| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East)
Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and ..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific)
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East)
Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
27.8
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM 1010K PEI
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM ATX200R PEI Blend (Europe-Africa-Middle East)
High flow Polyetherimide blend with internal mold release. RoHS compliant. UL94 V0 Listing.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East)
Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East)
Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Ultem AUT230M PEI (Europe-Africa-Middle East)
Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required...
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM HU1000 PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was ..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was ..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -50.0 - 50.0 °C
|
27.8
µin/in-°F <br>@Temperature -58.0 - 122 °F
|
2 |
|
Solvay Specialty Polymers Ryton® QC160N Polyphenylene Sulfide (PPS)
Ryton® QC160N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Ch..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -50.0 - 50.0 °C
|
27.8
µin/in-°F <br>@Temperature -58.0 - 122 °F
|
2 |
|
Solvay Specialty Polymers Ryton® QC160P Polyphenylene Sulfide (PPS)
Ryton® QC160P (pelletized) polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Chemical Resista..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC (Asia Pacific)
LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM 9090 PEI
Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM ATX200 PEI Blend (Europe-Africa-Middle East)
High flow Polyetherimide blend. RoHS compliant, UL94 V0 Listing.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM AUT210 PEI
Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM AUT210 PEI (Europe-Africa-Middle East)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific)
High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -40.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature -40.0 - 302 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
|
|||