| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
| Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.130 % | 0.130 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.31 % | 0.31 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 7.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, H358/30 | 115 MPa | 16700 psi | ISO 2039-1 |
| Tensile Strength at Break | 45.0 MPa | 6530 psi | 5 mm/min; ISO 527 |
| 48.0 MPa | 6960 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 5 mm/min; ASTM D638 |
| 60.0 MPa | 8700 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 7.0 % | 7.0 % | 5 mm/min; ISO 527 |
| 46 % | 46 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 4.7 % | 4.7 % | Type I, 5 mm/min; ASTM D638 |
| 5.0 % | 5.0 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 2.46 GPa | 357 ksi | 5 mm/min; ASTM D638 |
| 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 94.0 MPa | 13600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 3.12 GPa | 453 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 3.40 GPa | 493 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
| 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Unnotched | NB @Thickness 6.40 mm |
NB @Thickness 0.252 in |
ASTM D4812 |
| Izod Impact, Notched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*3; ISO 180/1A |
| 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
| NB | NB | 80*10*4; ISO 180/1U | |
| 130 kJ/m² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
80*10*4; ISO 180/1U | |
| Charpy Impact Unnotched | NB | NB | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
| NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU | |
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/2C | |
| 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 61.0 J @Temperature 23.0 °C |
45.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Taber Abrasion, mg/1000 Cycles | 11 | 11 | CS-17, 1 kg; SABIC Method |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| 46.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 84.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 84.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
| Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 136 °C | 277 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 136 °C | 277 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af | |
| 142 °C | 288 °F | Annealed 120°C, 2hrs; ISO 75/Ae | |
| 136 °C @Thickness 3.20 mm |
277 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
| 143 °C | 289 °F | Rate B/120; ISO 306 | |
| 154 °C | 309 °F | Rate B/50; ASTM D1525 | |
| UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
| UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ROA; IEC 60093 |
| Dielectric Constant | 2.8 @Frequency 1.00e+6 Hz |
2.8 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 2.9 @Frequency 50.0 - 60.0 Hz |
2.9 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
| 25.0 kV/mm @Thickness 1.60 mm |
635 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 | |
| 33.0 kV/mm @Thickness 0.800 mm |
838 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 | |
| Dissipation Factor | 0.0010 @Frequency 50.0 - 60.0 Hz |
0.0010 @Frequency 50.0 - 60.0 Hz |
IEC 60250 |
| 0.010 @Frequency 1.00e+6 Hz |
0.010 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
| 175 - 250 V | 175 - 250 V | UL 746A | |
| Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |