Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 6.35 mm |
291 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne LubriOne™ PC-20GF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PP HIP15025 HC Polypropylene Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Lexan® 3413R PC (Europe-Africa-Middle East) LEXAN 3413R is a high viscosity, 30% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Lexan® 3414R PC (Europe-Africa-Middle East) LEXAN 3414R is a high viscosity, 40% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Lexan® 505R PC (Europe-Africa-Middle East) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Lexan® XHT1143 PC (Europe-Africa-Middle East) XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP FARADEX DX92079 PC (Europe-Africa-Middle East) LNP* Faradex* DX92079 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Bead, Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding, Mold Release... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Lexan® XHT1141 PC (Asia Pacific) XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Lexan® XHT1141 PC (Europe-Africa-Middle East) XHT1141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1201-10 Polycarbonate Resin Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1301-12 Polycarbonate Resin Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 3010-10 Polycarbonate Resin Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 3030-10 Polycarbonate Resin Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1300-10 Polycarbonate Resin Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1303-10 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 3.20 mm |
291 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific) LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON DEL329EP PC (Europe-Africa-Middle East) LNP* STATKON* DEL329EP is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features include: Electrically Conductive, Internally Lubricated, Flame retard.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | annealed; ASTM D648 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Annealed; ISO 75-2/B |
Styron CALIBREâ„¢ 201-10 Polycarbonate Resin Overview: CALIBREâ„¢ 201-10 is produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. It provides excellent impact resistance, heat distortion resi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Annealed; ISO 75-2/B |
Styron CALIBREâ„¢ 301-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Unannealed; ASTM Data |
Styron CALIBREâ„¢ 5101 15 Polycarbonate, 10% Glass Reinforced CALIBRE 5101 is a 10% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5101 resin exhibits high modulus and excellent dimensional stability. CALIBRE 5101 .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Samyang Trirex® 3020PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020PJ is a high flow grade.Information provided by Samyang. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | 0.157 in, annealed; ASTM D648 |
Styron EMERGEâ„¢ 4330-10 Polycarbonate EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | annealed; ASTM D648 |
Styron EMERGEâ„¢ 4630-10 Polycarbonate EMERGEâ„¢ PC 4630-10 advanced resin is formulated to supply both excellent ultraviolet stability and enhanced ignition resistance while maintaining excellent physical properties and processabilit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON DEL359EF PC LNP* STAT-KON* DEL359EF is a compound based on Polycarbonate containing 25% Carbon Fiber, 15% PTFE. Added features include: Flame Retardant. Electrically Conductive, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ISO 75-1/-2 |
Covestro Makrolon® WB1239 Polycarbonate ISO 7391-PC,B,(,,)-05-9Global gradeMVR (300 °C/1.2 kg) 2.5 cm3/10 minBlow moldingHigh viscosityBranchedFood contact qualityExtrusion blow moldingInjection stretch blow moldingAvailable in transpare.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Aclo Accutech Polycarbonate POL051G10L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Aclo Accutech Polycarbonate POL051G20L Glass Reinforced |