| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ISO.93 DIN.53482 |
|
Omnia Plastica PTFE Polytetrafluoroethylene
A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.Features:Chemical: ..
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
|
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance ..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | DIN 53482 |
|
Qualchem Danamid AFGF-30 Polyamide 66, 30% Glass Fiber
Reinforced with glass fiberInformation provided by Qualchem Zrt.
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
|
SABIC Innovative Plastics Lexan® 503RS PC (Europe-Africa-Middle East)
LEXAN 503RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade.
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 93 |
|
Nilit FRIANYL B63 EO Raw extruded nylon 6 for injection molding
Raw extruded nylon 6 for injection molding, lubricated in surface.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | |
|
Fujipoly Industries Sarcon® 45Q Thin-Film QR
Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | ASTM D257 |
|
LG Chemical HI855HS PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | ASTM D257 |
|
LG Chemical HI855M PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093:1980-01 |
|
Global EPP PA 66E Extruded Polyamide 66
Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
|
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP
BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of ..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
|
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | ASTM D 257 |
|
SABIC Innovative Plastics PC0700 PC (Asia Pacific)
PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics PC1500 PC (Europe-Africa-Middle East)
PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | ASTM D 257 |
|
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East)
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
|
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 0
Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | DIN 53482 |
|
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry
Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
|
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA), 45% Glass Fiber
Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
|
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
|
Techmer ES HiFill® PA6/6 GF/B40 L 20% Glass Bead/Glass Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by Weight and Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation ..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
|
Techmer ES Plastiblend® PA6/10 BK Nylon 610
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
|
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific)
Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365.
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D149 |
|
Vicone High Performance Rubber VicoPoly™ 54A-Y Nylon 66
Information provided by Vicone
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
|
DSM Arnite® AV2 370 /B PET-35% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
|
DSM Arnite® TV4 240 PBT-20% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
|
Ensinger TECAPET™ PET Polyethylene Terephthalate (PET)
TECAPET™ PET is an unreinforced, semicrystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus,..
|
|||
| Volume Resistivity |
1.00e+15
ohm-cm <br>@Temperature 20.0 °C
|
1.00e+15
ohm-cm <br>@Temperature 68.0 °F
|
ASTM D257 |
|
Fainplast Compounds HAX HF 4022 Halogen Free PVC
General purpose
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | dry; IEC 93 |
|
Azoty Tarnow™ Tarnamid® T-27 Polyamide 6 - Natural
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechanical strength, rigidi..
|
|||
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 |
|
Addiplast Addinyl A2 ZP40 Nylon 66, 40% Mineral Filled
Mineral filled, increased thermal aging stabilityInformation provided by Addiplast.
|
|||
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
|
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
|
|||