Polymer Property : Flexural Modulus = 3.40 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.40 GPa

@Temperature 23.0 °C
493 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus 3.40 GPa

@Temperature 23.0 °C
493 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPHC GF3020 PB7 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® 500ECR PC
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® 503R PC (Europe-Africa-Middle East)
LEXAN 503R is a medium viscosity, 10% glass reinforced, UV-stabilized, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and exce..
Flexural Modulus 3.40 GPa
493 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® BFL2010 PC
Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors.
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based ..
Flexural Modulus >= 3.40 GPa
>= 493 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics LNP FARADEX NX07331 PC+ABS (Asia Pacific)
FARADEX NX07331 is a commercial grade EMI shielding material
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
Mitsubishi Xantar® G2F 23 UR Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Flexural Modulus 3.40 GPa
493 ksi
Conditioned; ISO 178
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers
PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp WFL32 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WFL32 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 3.40 GPa
493 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 4001 PEI (Asia Pacific)
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
Solvay Specialty Polymers Ryton® QC160N Polyphenylene Sulfide (PPS)
Ryton® QC160N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Ch..
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DFB03GR PC (Europe-Africa-Middle East)
LNP* THERMOCOMP* DFB03GR is a compound based on Polycarbonate resin containing a mixture of Glass Fiber and Glass Beads. Added features of this material include: Easy Molding.
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP KB003RXZ Acetal Copolymer
LNP THERMOCOMP* KB003RXZ is a compound based on Acetal Copolymer resin containing 15% Glass Bead. Added features of this material include: Easy Release.
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Noryl GTX GTX8110 PPE+PA (Europe-Africa-Middle East)
GTX8110 is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaksThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 3.40 GPa
493 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Asia Pacific)
PPE+PS blend. 10% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including wate..
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Unitika LM-8503-10
Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd.
Flexural Modulus >= 3.40 GPa
>= 493 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Flexural Modulus >= 3.40 GPa
>= 493 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Flexural Modulus >= 3.40 GPa
>= 493 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1220 Glass Filled Chemically Coupled Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1220 is a 20% glass filled chemically coupled impact copolymer polypropylene product.Information provided by A. Schulman.
Flexural Modulus 3.40 GPa
493 ksi
2mm/min; ISO 178
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Adell BJ-33 Nylon 6, 15% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Ashley Polymers Ashlene® 527-13G Nylon 66, 13% Glass Reinforced
A 13% glass reinforced, impact modified Nylon 66.Data provided by the manufacturer
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Adell BJ-13 Nylon 6, 15% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Flexural Modulus 3.40 GPa
493 ksi
2mm/min; ISO 178
Teijin Panlite® G-3410H Low Anisotropy, Glass Fiber Reinforced Polycarbonate Resin
Reinforced with 10 % of special GF and improved appearance grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPreci..
Flexural Modulus >= 3.40 GPa
>= 493 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Ashley Polymers Ashlene® P291WO PPO
A reinforced, flame retardant resin with outstanding structural strength. Good appearance and high impact.Data provided by the manufacturer
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer
Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based ..