| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics Cycolac® FR15 ABS
Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics Lexan® 3414R PC
40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics Lexan® 500 PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | surface, PLC code 4; UL 746A |
|
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific)
Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | surface, PLC code 4; UL 746A |
|
SABIC Innovative Plastics Lexan® ML5472 PC
Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2100 PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2100F PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing, WRAS certification in recognized colors..
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2100R PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2210R PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2310EPR PEI
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2310R PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2310R PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | surface, PLC code 4; UL 746A |
|
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi..
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2400 PEI
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2400 PEI (Asia Pacific)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2410 PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 2410R PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 3452 PEI (Asia Pacific)
45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM ATX200R PEI Blend (Europe-Africa-Middle East)
High flow Polyetherimide blend with internal mold release. RoHS compliant. UL94 V0 Listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | surface, PLC code 4; UL 746A |
|
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi..
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+PS
LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses).
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
|
|||
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses).
|
|||
| High Amp Arc Ignition, HAI | 0.00 arcs | 0.00 arcs | PLC Code; ASTM 746A |
|
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade
Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a..
|
|||
| High Amp Arc Ignition, HAI |
0.00
arcs @Thickness >=0.700 mm |
0.00
arcs @Thickness >=0.0276 in |
UL 746C |
|
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
|
|||