Mechanical Properties Metric English Comments
Flexural Modulus 3.40 GPa

@Temperature 23.0 °C
493 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB SCANMID 6 B12^ NH11L Nylon 6, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® 500ECR PC (Asia Pacific)
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East)
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® 500R PC (Europe-Africa-Middle East)
LEXAN 500R is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and excellent impact pe..
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® 505R PC (Europe-Africa-Middle East)
Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm...
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Ineos Nova 3930 General Purpose Crystal Polystyrene  (discontinued **)
High melt flow, Crystal clearApplications: Razor components, Personal care, Thin wall moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and ..
Flexural Modulus 3.40 - 9.32 GPa
493 - 1350 ksi
Average value: 6.32 GPa Grade Count:16
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Flexural Modulus 3.40 GPa
493 ksi
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer
Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 210E is most commonly used for thermoformed sheet applications.
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
Lucite International Diakon® CMH454 Acrylic Polymer
Information provided by Lucite International
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
Lucite International Diakon® Frost 952 51 Acrylic Polymer
Information provided by Lucite International
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Flexural Modulus 3.40 GPa
493 ksi
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Ineos ABS Lustran® SAN Sparkle Highest-Clarity
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RAL22 is a compound based on PA66 resin containing PTFE, Aramid Fiber. Added Features: Internally Lubricated
Flexural Modulus 3.40 GPa
493 ksi
DIN 53457
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry
Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp WFL32 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WFL32 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 3.40 GPa
493 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 4001 PEI
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 3.40 GPa
493 ksi
ISO 178
Solvay Specialty Polymers Ryton® QA200N Polyphenylene Sulfide (PPS)
Ryton® QA200N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal StabilityAdditional Pr..
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® 745 PBT (Europe-Africa-Middle East)
VALOX 745 is 30% mineral filled PBT injection moulding resin with improved toughness and low warpage. Applications: telephone ringer frames, card racks.
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Noryl GTX GTX8110P PPE+PA (Europe-Africa-Middle East)
GTX8110P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaksThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 3.40 GPa
493 ksi
.05 in/min;ASTM D790
Styrolution NAS® 90 High Performance Styrenic
NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla..
Flexural Modulus >= 3.40 GPa
>= 493 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Flexural Modulus 3.40 GPa
493 ksi
ASTM-D790
Polyram RamTal PM3009G5 Acetal, 25% Glass Fiber
25% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram Ram On Ind.
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1220 Glass Filled Chemically Coupled Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1220 is a 20% glass filled chemically coupled impact copolymer polypropylene product.Information provided by A. Schulman.
Flexural Modulus 3.40 GPa
493 ksi
2mm/min; ISO 178
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
Eurostar Starflam A28UL PA66, Flame Retardant, Injection Molding
Staramide A28UL is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Ashley Polymers Ashlene® PB1410 Polycarbonate, 10% Glass Reinforced
A 10% glass reinforced polycarbonate for increased mechanical strength and thermal properties. PB1413: with UV stabilizer.Data provided by the manufacturer
Flexural Modulus 3.40 - 7.30 GPa

@Temperature 120 - 200 °C
493 - 1060 ksi

@Temperature 248 - 392 °F
Average value: 5.26 GPa Grade Count:5
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Flexural Modulus 3.40 GPa
493 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer
Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based ..