Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Moisture Absorption 0.150 %
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.40 %
0.40 %
ISO 62
Viscosity 195000 cP
195000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
Melt Flow 22 g/10 min
<br>@Load 5.00 kg,<br> Temperature 260 °C
22 g/10 min
<br>@Load 11.0 lb,<br> Temperature 500 °F
ASTM D1238
Melt Index of Compound 21 g/10 min
<br>@Load 5.00 kg,<br> Temperature 260 °C
21 g/10 min
<br>@Load 11.0 lb,<br> Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 51.0 MPa
7400 psi
50 mm/min; ISO 527
52.0 MPa
7540 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 54.0 MPa
7830 psi
50 mm/min; ISO 527
55.0 MPa
7980 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 115 %
115 %
Type I, 50 mm/min; ASTM D638
115 %
115 %
50 mm/min; ISO 527
Elongation at Yield 4.5 %
4.5 %
50 mm/min; ISO 527
4.7 %
4.7 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.20 GPa
319 ksi
1 mm/min; ISO 527
2.30 GPa
334 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 83.0 MPa
12000 psi
2 mm/min; ISO 178
89.0 MPa
12900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
2 mm/min; ISO 178
2.30 GPa
334 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
4.80 J/cm
<br>@Temperature -30.0 °C
8.99 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*3; ISO 180/1A
45.0 kJ/m²
<br>@Temperature -30.0 °C
21.4 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 7.00 J/cm²
33.3 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
4.50 J/cm²
<br>@Temperature -30.0 °C
21.4 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 56.0 J
<br>@Temperature 23.0 °C
41.3 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
70.0 J
<br>@Temperature -30.0 °C
51.6 ft-lb
<br>@Temperature -22.0 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
259 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
107 °C
<br>@Thickness 3.20 mm
225 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 127 °C
261 °F
Rate B/50; ASTM D1525
127 °C
261 °F
Rate B/50; ISO 306
129 °C
264 °F
Rate B/120; ISO 306
UL RTI, Electrical 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical with Impact 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical without Impact 60.0 °C
140 °F
UL 746B
Flammability, UL94 HB
<br>@Thickness 1.50 mm
HB
<br>@Thickness 0.0591 in
UL 94
HB
<br>@Thickness 3.00 mm
HB
<br>@Thickness 0.118 in
UL 94
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-13
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Strength 17.0 kV/mm
<br>@Thickness 3.20 mm
432 kV/in
<br>@Thickness 0.126 in
in oil; IEC 60243-1
25.0 kV/mm
<br>@Thickness 1.60 mm
635 kV/in
<br>@Thickness 0.0630 in
in oil; IEC 60243-1
35.0 kV/mm
<br>@Thickness 0.800 mm
889 kV/in
<br>@Thickness 0.0315 in
in oil; IEC 60243-1
Descriptive Properties Value Comments
Ball Pressure Test, 75°C +/- 2°C Pass