| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled |
| Manufacturer | A. Schulman ComAlloy |
| Trade Name | Hiloy® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | A. Schulman ComAlloy Hiloy® 630 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced, UL.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.50 g/cc | 0.0542 lb/in³ | |
| Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength, Ultimate | 159 MPa | 23100 psi | ASTM D638 |
| Elongation at Break | 4.0 % | 4.0 % | ASTM D638 |
| Flexural Strength | 236 MPa | 34200 psi | ASTM D790 |
| Flexural Modulus | 11.1 GPa | 1610 ksi | ASTM D790 |
| Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 7.37 J/cm | 13.8 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 255 - 275 °C | 491 - 527 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 290 °C | 554 °F | Approximate middle barrel temperature. |