Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
SABIC F04660 High Density Polyethylene for Blown Film Applications Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp.. |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
Network Polymers NPP 50-1060 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® FXC810AL PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Alpine White colour effects. The colour package may effect performance.This data was.. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific) PC+ ABS Automotive applications |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2907 HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness, good top loading capability, high surface gloss.Applications: Protective sports equipment, safety helmets, high impact custom molding.. |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness.Applications: Tote boxes, beverage crates.Data provided by the manufacturer. |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersIn.. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
DuPont Bynel® 4003 Anhydride-Modified HDPE Adhesive Resin
(discontinued **) Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process.. |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
NOVA Chemicals Sclair® 69A HDPE Extrusion Resin
(discontinued **) Features: High tensile strength, better moisture barrier, better oil and solvent resistance, lower friction coefficient, lower brittleness temperature, better abrasion resistance, better temperature.. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate A, Loading 1 (10 N); ASTM D1525 |
Entec Hypel® PEHD.8/.962 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B; ISO 306 |
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
Ineos HP53-25-155 HDPE HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where appli.. |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Vicat Softening Point | 129 °C @Load 1.02 kg |
264 °F @Load 2.25 lb |
ISO 306 |
Borealis FL5580 High Density Polyethylene FL5580 is a high density polyethylene with an excellent combination of extrusion properties and moisture barrier properties. Applications: FL5580 has been developed especially for applications like.. |
|||
Vicat Softening Point | 129 °C | 264 °F | |
Covestro Bayblend® T 85 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
Vicat Softening Point | 129 °C | 264 °F | |
Covestro Bayblend® T 85 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
Vicat Softening Point | 129 °C | 264 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® T85 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 131°Chigh impact and notched impact strengthPreprocessingMax. Water content |
|||
Vicat Softening Point | 129 °C | 264 °F | 50°C/hr; 50N |
Arkema Group Orgalloy® RS 6000 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Vicat Softening Point | 129 °C | 264 °F | 50°C/hr; 50N |
Arkema Group Orgalloy® RS 6000TLA Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Vicat Softening Point | 129 °C @Load 1.02 kg |
264 °F @Load 2.25 lb |
ASTM D1525 |
Braskem Green PE SGF4950 Blow Molding and Monofilament High Density Polyethylene Description: SGF4950 is a high-density polyethylene copolymer, developed for the blow-molding segment. It shows well balanced properties between impact and stiffness, combined with high environmenta.. |
|||
Vicat Softening Point | 129 °C @Load 1.02 kg |
264 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem IE59U3 HDPE Injection Molding Polyethylene Homopolymer IE59U3 is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for injection molding applications. It offers high stiffness and impact strength, good pro.. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer 40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Vicat Softening Point | 129 °C | 264 °F | 50°C/hr; 50N |
Arkema Group Orgalloy® R 60ES Nylon 6 Alloy (Conditioned) Rigid polyamide 6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents). Blow extrusion grade for technical films: thermal resistance, barrier to gases and aromas,.. |