Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS (Asia Pacific) PC/ABS with high stiffness and impact performance |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS PC+ ABS Automotive applications |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANLON A 5005B UV PA/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific) CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 178 |
LG Chemical Lupoy 1621-02 Polycarbonate Resin Description: LUPOY PC 1621-02 resin is designed for large injection stretch blow molding and extrusion blow molding parts. It exhibits an excellent physical property balance of heat resistance, tran.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179 |
Iran Petrochemical (PCC) BL7 HM 6255 High Density Polyethylene BL7 (HM 6255) is a high density polyethylene with Butene-1 as comonomer. It is a special grade for particularly high requirements like low temperature impact strength and stacking, good stress crack.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179-1/1eA |
Styron INSPIREâ„¢ TF0808S(U) Polypropylene TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE .. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX964 PPE+PA (Europe-Africa-Middle East) NORYL GTX964 is an unfilled impact modified material with optimised processability. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PC Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW441 (COND) Nylon 46 High Viscosity, Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60 Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60 Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following .. |
|||
Charpy Impact, Notched | 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60 Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following .. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TSZ 1 PA666 Product description: Grilon TSZ 1 is a heat stabilized, normal viscosity, impact modified PA66 + PA6 injection molding grade. Grilon TSZ 1 has the following important properties: Excellent flow beha.. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | |
BASF Novolen® 2500 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | |
BASF Novolen® 2600 M Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |