Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 12.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 920 PC
Opaque colors, low viscosity, superior flame retardance.
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 923A PC
Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized.
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 940ASR PC (Asia Pacific)
More robust design of standard 900 series flame retardant grade. Internal mold release.
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 943ASR PC (Asia Pacific)
More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized.
Izod Impact, Notched 6.41 J/cm

@Temperature 22.8 °C
12.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow
Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co..
Izod Impact, Notched 6.41 J/cm

@Temperature 22.8 °C
12.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Izod Impact, Notched 6.41 J/cm

@Temperature 22.8 °C
12.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow
Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted..
Izod Impact, Notched 6.41 J/cm

@Temperature 22.8 °C
12.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Izod Impact, Notched 6.41 J/cm

@Temperature 22.8 °C
12.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow
Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc..
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D256
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
natural, tints; ASTM D256
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Izod Impact, Notched 6.38 J/cm

@Temperature -30.0 °C
12.0 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® ML7693 PC Copolymer (Asia Pacific)
Medium-flow impact-modified high-flow-ductile PC copolymer. Available in black color only.
Izod Impact, Notched 6.40 J/cm

@Thickness 6.40 mm
12.0 ft-lb/in

@Thickness 0.252 in
ASTM D256
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
Izod Impact, Notched 6.40 J/cm

@Thickness 6.40 mm
12.0 ft-lb/in

@Thickness 0.252 in
ASTM D256
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
Izod Impact, Notched 6.40 J/cm

@Thickness 6.40 mm
12.0 ft-lb/in

@Thickness 0.252 in
ASTM D256
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® HF1140 PC (Europe-Africa-Middle East)
Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this..
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® ML4539 PC
Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Injection moldable. Opaque colors.
Izod Impact, Notched 6.40 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Lucent Polymers PC/ABS-1208 Polycarbonate+ABS, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 6.41 J/cm

@Temperature 23.0 °C
12.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
MRC Polymers NAXALOYâ„¢ 770-NT172 ABS + PC Alloy
Information provided by MRC Polymers Inc.
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
LW; ASTM D256
Haysite H1000 Polyester Laminate
Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide..
Izod Impact, Notched 6.40 J/cm

@Temperature 23.0 °C
12.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S..
Izod Impact, Notched 6.40 J/cm

@Thickness 3.20 mm
12.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 2205 Polycarbonate, Injection Grade
Exceptionally good flow injection molding grade with easy mold release, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015, Bayer MaterialSc..
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
12.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers DIAMALOY 173U PC/Polyester Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 6.40 J/cm

@Temperature 23.0 °C
12.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics PC2200 PC
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
Copyright © lookpolymers.com All Rights Reserved