| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| SABIC Innovative Plastics Lexan® LUX2489D PC (Europe-Africa-Middle East) Lexan LUX2489D is a polycarbonate resin with high reflective properties, UV additive, medium viscosity, injection molding grade exhibiting low dust attraction. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| SABIC Innovative Plastics LNP Colorcomp D10009 PC LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Asia Pacific) Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® HP4 PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® VR2020 PC (Europe-Africa-Middle East) VR2020 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| SABIC Innovative Plastics PC0700 PC PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| SABIC Innovative Plastics PC0800 PC (Asia Pacific) PC0800 resin is a low flow (MFR = 8 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics PC1000 PC PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics PC1003R PC PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was .. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| SABIC Innovative Plastics PC1500 PC (Europe-Africa-Middle East) PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| SABIC Innovative Plastics PC1800 PC PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics PC6300 PC PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Americas region. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| SABIC Innovative Plastics PC6300 PC (Asia Pacific) PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| SABIC Innovative Plastics PC6300 PC (Asia Pacific) PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||