Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.26 g/cc | 1.26 g/cc | ASTM D792 |
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
Water Absorption | 0.10 % @Time 86400 sec |
0.10 % @Time 24.0 hour |
ASTM D570 |
Moisture Absorption | 0.0100 % | 0.0100 % | 50% RH, 24 hrs; ASTM D570 |
0.0100 % | 0.0100 % | 23°C / 50% RH; ISO 62 | |
Water Absorption at Saturation | 0.090 % | 0.090 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
Melt Flow | 17.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
17.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
Melt Index of Compound | 14 g/10 min @Load 5.00 kg, Temperature 220 °C |
14 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 50.0 MPa | 7250 psi | Type I, 5 mm/min; ASTM D638 |
50.0 MPa | 7250 psi | 5 mm/min; ISO 527 | |
Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D638 |
65.0 MPa | 9430 psi | Type I, 5 mm/min; ASTM D638 | |
Elongation at Break | 15 % | 15 % | 50 mm/min; ISO 527 |
100 % | 100 % | Type I, 5 mm/min; ASTM D638 | |
Elongation at Yield | 3.5 % | 3.5 % | 5 mm/min; ISO 527 |
4.0 % | 4.0 % | Type I, 5 mm/min; ASTM D638 | |
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
3.50 GPa | 508 ksi | 5 mm/min; ASTM D638 | |
Flexural Yield Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Flexural Modulus | 3.30 GPa | 479 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
3.45 GPa | 500 ksi | 2 mm/min; ISO 178 | |
Izod Impact, Notched | 2.00 J/cm | 3.75 ft-lb/in | ASTM D256 |
0.880 J/cm @Temperature -30.0 °C |
1.65 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
Izod Impact, Notched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*3; ISO 180/1A |
5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
Dart Drop, Total Energy | 50.0 J @Temperature 23.0 °C |
36.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
Deflection Temperature at 0.46 MPa (66 psi) | 97.0 °C @Thickness 6.40 mm |
207 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
83.0 °C @Thickness 3.20 mm |
181 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
Vicat Softening Point | 91.0 °C | 196 °F | Rate B/50; ASTM D1525 |
98.0 °C | 208 °F | Rate B/50; ISO 306 | |
102 °C | 216 °F | Rate B/120; ISO 306 | |
Flammability, UL94 | V-1 @Thickness 0.600 mm |
V-1 @Thickness 0.0236 in |
UL 94 |
V-0 @Thickness 0.800 mm |
V-0 @Thickness 0.0315 in |
UL 94 | |
5VB @Thickness 1.50 mm |
5VB @Thickness 0.0591 in |
UL 94 | |
Glow Wire Test | 800 °C | 1470 °F | IEC 60695-2-13 |
850 °C | 1560 °F | IEC 60695-2-13 | |
960 °C @Thickness 0.800 mm |
1760 °F @Thickness 0.0315 in |
IEC 60695-2-12 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.68e+16 ohm-cm | 2.68e+16 ohm-cm | ASTM D257 |
Surface Resistance | 3.54e+15 ohm | 3.54e+15 ohm | ASTM D257 |
Descriptive Properties | Value | Comments |
---|---|---|
Ball Pressure Test, 75°C +/- 2°C | PASSES | IEC 60695-10-2 |