| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Cycolac® GX3800F ABS
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific)
Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East)
Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® 943X PC Copolymer
Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Asia Pacific)
Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRILOY D2000 PC
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific)
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific)
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics LNP STAT-KON TD000 PU
LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive.
|
|||
| Dart Drop, Total Energy | 50.0 J | 36.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific)
Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Europe-Africa-Middle East)
NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics NORYL N190X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Asia Pacific)
Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The ..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Europe-Africa-Middle East)
Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The ..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific)
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East)
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
|
|||
| Dart Drop, Total Energy |
50.0
J @Temperature 23.0 °C |
36.9
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
|
|||