| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled |
| Manufacturer | Polykemi AB |
| Trade Name | POLYabs |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Polykemi AB POLYabs F00 GF17 ABS, Glass Fiber-Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
| Filler Content | 17 % | 17 % | ±2%; Polykemi |
| Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | Across Flow; ISO 2577 |
| 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | With Flow; ISO 2577 | |
| Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 42.0 MPa | <= 6090 psi | ISO/R527 |
| Elongation at Break | 4.5 % | 4.5 % | ISO/R527 |
| Flexural Strength | <= 73.0 MPa | <= 10600 psi | ISO 178 |
| Flexural Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| 110 °C @Load 1.00 kg |
230 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 190 - 230 °C | 374 - 446 °F | |
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
| Drying Temperature | 80.0 °C | 176 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
| 2 - 4 hour | 2 - 4 hour | in fresh-air dryer | |
| 2 - 4 hour | 2 - 4 hour | in circulation dryer | |
| Injection Pressure | 90.0 - 150 MPa | 13100 - 21800 psi | |
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | 20-40 | % of injection pressure |
| Injection Speed () | High |