| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs N30 ABS
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs S00 GK10 ABS, High Flow
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs S20 ABS
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs SN0 ABS
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs SS0 GK10 ABS, High Flow
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYasa 2410F High Flow ASA
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYblend 50LG PC/ABS-Blend, Low Gloss
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYblend 65 M10 PC/ABS-blend, Reinforced
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYblend 65FS GF20 PC/ABS-Blend
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYblend 65H PC/ABS-Blend
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYblend 85H PC/ABS-Blend
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYblend 90VB PC/ABS-Blend, Flame Retardant
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYblend C65HF PC/ABS-blend
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYelast TPE EZ506X Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYelast TPE S902A Thermoplastic Elastomer, SBS-based
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYelast TPE Z500 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYelast TPE Z900 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYfill PP CIP15015 UV Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYfill PP CQX10030E10 F Polypropylene, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYfill PPC T4030 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs F00 GF15 ABS, Glass Fiber-Reinforced
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs F00L ABS
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs F20 ABS
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs HD2 ABS
Information provided by Polykemi AB
|
|||
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi | |
|
Polykemi AB POLYabs HH0 ABS, Extra Heat Resistance
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYelast TPE Z606 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
|
|||
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
|
Polykemi AB POLYelast TPE Z557 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||