Polymer Property : Injection Pressure = 21800 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Plastcom SLOVAMID 6 GF 60 Polyamide 6, 60% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 60% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYabs N00 LG ABS, Low Gloss
Information provided by Polykemi AB
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYabs S00 GK10 ABS, High Flow
Information provided by Polykemi AB
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYabs S20 ABS
Information provided by Polykemi AB
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYabs V0X ABS, Flame Retardant
Information provided by Polykemi AB
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYasa 1614F UV-resistant ASA
Information provided by Polykemi AB
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYblend 45V GF10 PC/ABS-blend, Flame Retardant
Information provided by Polykemi AB
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYblend 45V PC/ABS-blend, Flame Retardant
Information provided by Polykemi AB
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYblend 85 M10 PC/ABS-Blend
Information provided by Polykemi AB
Injection Pressure 50.0 - 150 MPa
7250 - 21800 psi
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral  (discontinued **)
Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical..
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYabs HF0 ABS
Information provided by Polykemi AB
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Polykemi AB POLYabs F00 GF17 ABS, Glass Fiber-Reinforced
Information provided by Polykemi AB