Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 221 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYabs SS0 GK10 ABS, High Flow
Information provided by Polykemi AB
Vicat Softening Point 105 °C

@Load 5.001 kg
221 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYblend 45FS GKF2010 PC/ABS-Blend, Glass Fiber reinforced
Information provided by Polykemi AB
Vicat Softening Point 105 °C

@Load 5.001 kg
221 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANLON A 5005 PA/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 105 °C

@Load 5.001 kg
221 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANLON A 5005B PA/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 105 °C

@Load 5.001 kg
221 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANLON A 5005B UV PA/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYabs F00 ABS
Information provided by Polykemi AB
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
120°C/min; ASTM D1525
Kingfa HR-527 Modified ABS
Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 105 °C

@Load 1.02 kg
221 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Luran® S 767KE ASA
Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos..
Vicat Softening Point 105 °C

@Load 5.10 kg
221 °F

@Load 11.2 lb
50°C/h; ISO 306
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled
Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro..
Vicat Softening Point 105 °C

@Load 1.02 kg
221 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Terlux® HD 2822 MABS
Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well ..
Vicat Softening Point 105 °C

@Load 5.10 kg
221 °F

@Load 11.2 lb
ISO 306
Borealis PS65C40 Polypropylene Compound, Mineral Filled
PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and..
Vicat Softening Point 105 °C

@Load 0.999 kg
221 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND 4500 V0 HF Flame Retardant PC - ABS
PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, excellent mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 105 °C

@Load 5.00 kg
221 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0417 GIF Acrylonitrile Butadiene Styrene, 17% Glass Filled
ABS with 17% glass fiber reinforcementGood thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 105 °C

@Load 5.00 kg
221 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 3510 HT Acrylonitrile Butadiene Styrene
ABS with very high impact resistanceHigh impact resistance at low temperature, high heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 105 °C

@Load 0.999 kg
221 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 3520 Acrylonitrile Butadiene Styrene
ABS with high impact resistanceHigh melt flow rate, high impact resistance at low temperature, excellent processability and surface appearanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Kibilac® PW-957 ASA Polymer
Injection
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Kibilac® PW-997S ASA Polymer
Extrusion
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Kibisan® PN-106 L150 SAN
High Clarity
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Kibisan® PN-107 L125 SAN
High Clarity
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-717C ABS
Medium impact
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PH-888G Polystyrene - High gloss
High impact; high gloss
Vicat Softening Point 105 - 110 °C

@Load 5.00 kg
221 - 230 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-727 ABS
Electro-plating
Vicat Softening Point 105 °C

@Load 5.00 kg
221 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-747F ABS - Extrusion
Refrigerator
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-757 ABS
High gloss, medium impact
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-758R ABS - Transparent
Transparent, Chemical Resistant
Vicat Softening Point 105 °C

@Load 5.00 kg
221 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-777B ABS - High Heat
High Heat Impact
Vicat Softening Point 105 °C

@Load 1.00 kg
221 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-763A ABS - Flame Retardant
F.R. High Heat
Vicat Softening Point 105 °C

@Load 5.001 kg
221 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs F00 GF17 ABS, Glass Fiber-Reinforced
Information provided by Polykemi AB
Vicat Softening Point 105 °C

@Load 5.10 kg
221 °F

@Load 11.2 lb
50°C/hour; ISO 306
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
Copyright © lookpolymers.com All Rights Reserved