Polymer Property : Mold Temperature = 60.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Plastcom SLOVAMID 66 GF 15 TS PA66, 15% glass fibre
FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Polykemi AB POLYabs T00 ABS, Transparent
Information provided by Polykemi AB
Mold Temperature 60.0 °C
140 °F
Injection Molding
Ineos ABS Centrex® 601 ASA+AES Blend  (discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionInformation..
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Injection Molding
LG Chemical LUCEL N109WR POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Injection Molding
LG Chemical LUCON 6080EX ABS+CF
Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio..
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Injection Molding
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Solvay TECHNYL® B 238 Black 21 N PA66/6, DRY
Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular..
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY
Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and..
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Solvay TECHNYL® 27010ST PA66, DRY
Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of..
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Borealis Nepol™ GB303HP 30% Long Glass Fiber Reinforced Polypropylene
Nepol GB303HP is a 30% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th..
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch..
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded
AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded
BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Eurostar Starflam P10002E PA6, Injection Molded
Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec..
Mold Temperature 60.0 - 110 °C
140 - 230 °F
Eurotec® Tecodur® PB70 GR20 BK002 TD21 PBT/PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), impact modified, natural
Information provided by Eurotec®
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Mold Temperature 60.0 °C
140 °F
for shrinkage test, Optimal
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT
Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic ..
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Beijing Ranger Chem PBT-201-G20 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Beijing Ranger Chem PBT-MFC-G20 FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Mold Temperature 60.0 - 100 °C
140 - 212 °F
BASF Ultradur S 4090 G4 20% Glass Filled PBT
Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio..
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Injection-molding
BASF Ultraform® W2320 0035 POM
Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Injection-molding
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Conditioned)
Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire ..
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Beijing Ranger Chem PBT-201-G30 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Mold Temperature 60.0 °C
140 °F
for shrinkage test
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT
Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs..