| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Dry Time | 2 hour | 2 hour | |
|
Multibase Multi-Pro® 2516 CU Polypropylene
Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult..
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
|
Multibase TPSiV® 3111-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Hydrolysis resistant; FDA 21 CFR 177.2600 CompliantAPPLICATIONS: Solution for soft touc..
|
|||
| Dry Time | 2 - 8 hour | 2 - 8 hour | in fresh-air dryer |
|
Polykemi AB POLYblend C65HF PC/ABS-blend
Information provided by Polykemi AB
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
|
Polykemi AB POLYfill PP HIP15025 HC Polypropylene
Information provided by Polykemi AB
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
|
Polykemi AB POLYfill PPH GF15020 PD1 NBR PP, Glass Fiber-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
|
Ravago Manufacturing Americas Hylon® N1000THL Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
|
Polykemi AB POLYfill PPH BK901010 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
|
Polykemi AB POLYfill PPH T3022D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant
Information provided by Polykemi AB
|
|||
| Dry Time | 2 hour | 2 hour | Drying not normally required |
|
Fiberfil® J-68/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
|
Star Plastics ABSLG5035 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Pre-drying |
|
Styrolution Luran® S 757 R Colored ASA
Description: General-purpose grade for injection molding with high stiffness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Pre-drying |
|
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
|
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
|
A. Schulman SCHULADUR® A GF33HI 33% Glass Fiber Reinforced, High Impact PBT
Information provided by A. Schulman.
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
|
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6
Information provided by A. Schulman.
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
|
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Opened bags and gaylord boxes |
|
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
|
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Option 3 |
|
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE.
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
|
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6
Information provided by A. Schulman.
|
|||
| Dry Time | 2 hour | 2 hour | |
|
Ecomass® 4710BI71 Filled Polyurethane, Injection Molding
Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead for weighting, balancing and vibration..
|
|||
| Dry Time |
2
-
4
hour <br>@Temperature 71.1 °C
|
2
-
4
hour <br>@Temperature 160 °F
|
to eliminate surface defects |
|
Clariant Renol PBT1100S Polybutylene Terephthalate, Silicone Lubricated
Data provided by Clariant Masterbatches
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
|
BASF Petra® 7010 BK 5830 15% Glass Filled PET
Description: Petra 7010 BK5830 is a 15% glass fiber reinforced, pigmented black injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface ..
|
|||
| Dry Time | 2 - 16.0 hour | 2 - 16.0 hour | |
|
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
|
Polykemi AB POLYabs F00 GF17 ABS, Glass Fiber-Reinforced
Information provided by Polykemi AB
|
|||