Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Arc Resistance = 60.0 sec Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Arc Resistance 60.0 - 120 sec
60.0 - 120 sec
ASTM D495
Raschig Group DECAL® 2061 Phenolic
Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and ..
Arc Resistance 60.0 - 120 sec
60.0 - 120 sec
ASTM D495
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 117 sec Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 117 sec Grade Count:17
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 137 sec Grade Count:14
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Arc Resistance 60.0 - 120 sec
60.0 - 120 sec
Average value: 90.0 sec Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Arc Resistance 60.0 - 120 sec
60.0 - 120 sec
Average value: 81.4 sec Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 107 sec Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
Arc Resistance 60.0 - 120 sec
60.0 - 120 sec
Average value: 81.7 sec Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Arc Resistance 60.0 - 120 sec
60.0 - 120 sec
Average value: 114 sec Grade Count:9
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 121 sec Grade Count:4
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 105 sec Grade Count:8
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Arc Resistance 60.0 sec
60.0 sec
Average value: 60.0 sec Grade Count:3
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 105 sec Grade Count:4
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Arc Resistance 60.0 - 193 sec
60.0 - 193 sec
Average value: 163 sec Grade Count:5
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
Arc Resistance 60.0 - 120 sec
60.0 - 120 sec
Average value: 83.0 sec Grade Count:5
Overview of materials for Phenolic, Novolac, Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu..
Arc Resistance 60.0 - 179 sec
60.0 - 179 sec
Average value: 108 sec Grade Count:20
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Arc Resistance 60.0 - 179 sec
60.0 - 179 sec
Average value: 121 sec Grade Count:9
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Arc Resistance 60.0 - 179 sec
60.0 - 179 sec
Average value: 115 sec Grade Count:7
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 124 sec Grade Count:6
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Arc Resistance 60.0 - 130 sec
60.0 - 130 sec
Average value: 119 sec Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 110 sec Grade Count:3
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 120 sec Grade Count:5
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..