Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Arc Resistance = 179 sec Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Arc Resistance 30.0 - 179 sec
30.0 - 179 sec
Average value: 116 sec Grade Count:18
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Arc Resistance 60.0 - 179 sec
60.0 - 179 sec
Average value: 108 sec Grade Count:20
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM
Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM
Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, ..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM
Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D496
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
Arc Resistance 60.0 - 179 sec
60.0 - 179 sec
Average value: 115 sec Grade Count:7
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM
Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded
Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo..
Copyright © lookpolymers.com All Rights Reserved