| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 60.0 - 120 sec | 60.0 - 120 sec | ASTM D495 |
| Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
| Arc Resistance | 60.0 - 120 sec | 60.0 - 120 sec | ASTM D495 |
| Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 117 sec Grade Count:14 |
| Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 117 sec Grade Count:17 |
| Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 137 sec Grade Count:14 |
| Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
| Arc Resistance | 60.0 - 120 sec | 60.0 - 120 sec | Average value: 90.0 sec Grade Count:14 |
| Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
| Arc Resistance | 60.0 - 120 sec | 60.0 - 120 sec | Average value: 81.4 sec Grade Count:7 |
| Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 107 sec Grade Count:3 |
| Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
| Arc Resistance | 60.0 - 120 sec | 60.0 - 120 sec | Average value: 81.7 sec Grade Count:3 |
| Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
| Arc Resistance | 60.0 - 120 sec | 60.0 - 120 sec | Average value: 114 sec Grade Count:9 |
| Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 121 sec Grade Count:4 |
| Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 105 sec Grade Count:8 |
| Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
| Arc Resistance | 60.0 sec | 60.0 sec | Average value: 60.0 sec Grade Count:3 |
| Overview of materials for Polyarylamide, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values.. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 105 sec Grade Count:4 |
| Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
| Arc Resistance | 60.0 - 193 sec | 60.0 - 193 sec | Average value: 163 sec Grade Count:5 |
| Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
| Arc Resistance | 60.0 - 120 sec | 60.0 - 120 sec | Average value: 83.0 sec Grade Count:5 |
| Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
| Arc Resistance | 60.0 - 179 sec | 60.0 - 179 sec | Average value: 108 sec Grade Count:20 |
| Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
| Arc Resistance | 60.0 - 179 sec | 60.0 - 179 sec | Average value: 121 sec Grade Count:9 |
| Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
| Arc Resistance | 60.0 - 179 sec | 60.0 - 179 sec | Average value: 115 sec Grade Count:7 |
| Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 124 sec Grade Count:6 |
| Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
| Arc Resistance | 60.0 - 130 sec | 60.0 - 130 sec | Average value: 119 sec Grade Count:12 |
| Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 110 sec Grade Count:3 |
| Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 120 sec Grade Count:5 |
| Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||