Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.03 g/cc | 0.0372 lb/in³ | NCMT Method |
NCMT NanoPAC™ HS402 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | NCMT Method |
NCMT NanoPAC™ S203 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Electrical Appliances AutomobileInformation provided by Nano Composi.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | Liquid Property |
Fibre Glast 1110 L Vinyl Ester Resin (Laminate Properties) #1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM-D792 |
Ineos ABS Lustran® 786 ABS, Extrusion Grade Lustran® ABS 786 resin is a black, virgin extrusion grade of ABS (acrylonitrile butadiene styrene). It is designed for extruded drain, waste, and vent (DWV) pipe. Lustran® ABS 786 (901046 blac.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ISO 1183 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Europe-Africa-Middle East) LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA11 GL8 HS UV Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Graphite Powder Lubricant and UV StabilizerFeatures: Heat Stabilized. Good UV Resistance and LubricatedAppearance: Natural ColorIn.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Spartech Royalite R84 Proprietary Polymer Weather Resistant Sheet Data provided by the manufacturer. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ISO 1183 |
Styrolution Terluran® EGP-7 ABS Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Solvay LUBRHOPHOS® LB 400 E Surfactant Identification: ETHOXYLATED OELYL-CETYL ALCOHOL, PHOSPHATE ESTERSolubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and No.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific) LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM-D792 |
Polyram Polytron P20B01 Homopolymer Polypropylene, Chemically Coupled 20% Long Fiber A CHEMICALLY COUPLED 20% LONG FIBER GLASS REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | Melt |
Covestro Desmopan® DP 2792A Polyurethane Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content |
|||
Density | 1.03 g/cc @Temperature 270 °C |
0.0372 lb/in³ @Temperature 518 °F |
Melt |
Covestro Makroblend® DP 7645 Polycarbonate + PET, Impact Grade Developmental productISO 7792-PC/PET,MHPR,-020(PC/PET)-blends, impact modifiedInjection molding gradeunreinforcedPreprocessingMax. Water content |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ISO 1183 |
Chi Mei Polylac® PA-709 ABS Super impact |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Dow BETAFOAM™ 87124 Polyether / Polyol Blend BETAFOAM™ 87124 is a component used to make high-density, all-water blown rigid polyurethane foam.Information provided by Dow |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® L 25 W 40 PA12 Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid .. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ISO 1183 |
Arkema Group ORGASOL® 2002 EXD Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Density | 1.03 - 1.06 g/cc | 0.0372 - 0.0383 lb/in³ | Spec; ISO 1183-1 |
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer CP0437C20L Calcium Reinforced |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | Sintered; ASTM D792 |
ALM TPE-210-S Prototyping Polymer A thermoplastic elastomer used to produce parts with “rubber like” qualities. TPE 210-S exhibits good feature definition and infiltration with polyurethane will impart even higher toughness and ab.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
3M Scotchcast™ 2104 Electrical Insulating Resin Scotchcast 2104 Electrical Insulating Resin is a hard, two-part, polyurethane resin encapsulant designed especially for permanent splice protection. 2104 is formulated for virtually every electrical.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
3M Scotchgard™ Resilient Floor Protector Scotchgard Resilient Floor Protector is a high performance protective floor coating for vinyl tile and vinyl sheet flooring that utilizes multiple polymer technologies to produce a hard surface that.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Blue River Coatings Acrylic 4000D Topcoat BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Arkema Group Rilsan® BMF Nylon 11 (Conditioned) Designation ISO 1874-PA11,M,12-010Rigid grade for injection molding. Available color: natural. Additive free.Good melt viscosity. Outstanding ability to mold part with high length-thickness ratio an.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Conditioned) Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold... |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer CP0436M20L Mica Reinforced |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 15 MFI Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Solvay RHODASURF® TR/15-40 Surfactant Identification: WATER SOLUTION OF ETHOXYLATED TRIDECYL ALCOHOLCAS: 9043 – 30 – 5 ; 7732 – 18 – 5Solubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Available in:.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient.. |