Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.255 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.255 GPa
37.0 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips 1400 Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Good Flexibility, Good Flow, Good Warping Resistance, Good Mold Release, Good ESCRApplications:Lids & Closures, C..
Flexural Modulus 0.255 - 12.4 GPa
37.0 - 1800 ksi
Average value: 2.85 GPa Grade Count:99
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Flexural Modulus 0.255 - 36.2 GPa
37.0 - 5250 ksi
Average value: 6.54 GPa Grade Count:334
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Flexural Modulus 0.255 GPa
37.0 ksi
ASTM D790
LyondellBasell Petrothene® NA831000 Low Density Polyethylene
ApplicationsPETROTHENE NA831-000 resin exhibits high stress crack resistance and low temperature brittleness. Typical applications include housewares, containers and industrial parts. Regulatory St..
Flexural Modulus 0.255 GPa
37.0 ksi
ASTM D790
Techmer ES HiFill FR® PA6/6 FR 346 RD
Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc.
Flexural Modulus 0.255 GPa
37.0 ksi
ASTM D790
Lubrizol Estane® ALR E60D Thermoplastic Polyurethane
Type: Estane® ALR E60D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..
Flexural Modulus 0.255 GPa
37.0 ksi
ASTM D790
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Flexural Modulus 0.255 GPa
37.0 ksi
XD; ASTM D790
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..
Flexural Modulus 0.255 GPa
37.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman D4041-P Polyethylene  (discontinued **)
Low-density polyethylene D4041-P is a recommended for use in the boardstock coating industry for applications such as breadboard, cupstock, and liquid packaging board. This resin has low neck-in an..