| Category | Polymer , Thermoplastic , ABS Polymer |
| Manufacturer | LTL Color Compounds |
| Trade Name | ColorFast® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | LTL Color Compounds ColorFast® GPA300X ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | 0.125; ASTM D955 |
| Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 105 | 105 | ASTM D785 |
| Tensile Strength at Break | 27.6 MPa | 4000 psi | 2.0 in/min; ASTM D638 |
| Tensile Strength, Yield | 35.9 MPa | 5200 psi | 2.0 in/min; ASTM D638 |
| Elongation at Break | 110 % | 110 % | 2.0 in/min; ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | 2.0 in/min; ASTM D638 |
| Flexural Strength | 51.7 MPa | 7500 psi | 2.0 in/min; ASTM D790 |
| Flexural Modulus | 1.72 GPa | 250 ksi | 2.0 in/min; ASTM D790 |
| Izod Impact, Notched | 4.27 J/cm @Temperature 22.8 °C |
8.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | Unannealed (0.250"); ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
| Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
| Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
| Nozzle Temperature | 218 - 260 °C | 425 - 500 °F | |
| Melt Temperature | 218 - 260 °C | 425 - 500 °F | |
| Mold Temperature | 48.9 - 71.1 °C | 120 - 160 °F | |
| Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | nominal; maximum drying time of 8 hours |
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
| Shot Size | 30 - 60 % | 30 - 60 % | |
| Vent Depth | 0.00381 - 0.00508 cm | 0.00150 - 0.00200 in | |
| Screw Speed | 30 - 60 rpm | 30 - 60 rpm |