Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0080 in/in Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
Polycasa XT PMMA
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing..
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
Across Flow; ISO 2577
Polykemi AB POLYabs S00 ABS, High Flow
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
With Flow; ISO 2577
Polykemi AB POLYabs HF0 ABS
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
24 hours; ASTM D-955
Chevron Phillips MC3200 Crystal Polystyrene  (discontinued **)
High heat crystal polystyrene.Applications:Medical partsConsumer containers, vials, jars, etc.Clock lensesAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat softening tempera..
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact
Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica..
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
LyondellBasell SEQUEL® E3000 FR TPO
Description: SEQUEL® E3000FR thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is spe..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Lehmann & Voss LUVOCOM® 1106-8087/BL Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Lehmann & Voss LUVOCOM® 1301-7662/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Lehmann & Voss LUVOCOM® 1301-8386 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
0.125; ASTM D955
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded
13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc.
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Lucite International Diakon® CRG800 Acrylic Polymer, Toughened Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Lehmann & Voss LUVOCOM® 1106-8232 Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Linear Mold Shrinkage 0.0030 - 0.0080 cm/cm
0.0030 - 0.0080 in/in
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ISO 294-4
Styrolution Novodur® E211 ABS
Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ISO 294-4
Styrolution Novodur® E401 ABS
Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
<br>@Thickness 3.20 mm,<br> Time 259000 sec
0.0060 - 0.0080 in/in
<br>@Thickness 0.126 in,<br> Time 72.0 hour
ISO 294
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Diamond Polymers ABSPC 9901 ELG ABS/PC Injection Molding Grade, Very High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Diamond Polymers ASA S210B
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Diamond Polymers ASA TWP 155
Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Americas Styrenics EC6600 High Impact Polystyrene
Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toy..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Beijing Chemical Industry KAIFA® 304-G20 PBT Resin
20% glass fiber reinforced, flame retardant, low bleeding, UV-resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Americas Styrenics STYRON® 487 High Impact Polystyrene
Product CharacteristicsGood TrimmabilityToughnessHeat resistanceFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by A..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Americas Styrenics STYRON® 649D High Heat Crystal Polystyrene
Product CharacteristicsExcellent moldabilityExcellent gloss in coextrusionExcellent clarityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk ..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin
30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Beijing Chemical Industry KAIFA® MN301-G20 Nylon 66 Resin
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
0.125; ASTM D955
LTL Color Compounds ColorFast® GPA300X ABS
Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc.
Copyright © lookpolymers.com All Rights Reserved