Processing Properties Metric English Comments
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
PolyOne Nymax™ 600 A Zip 43 Natural Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
PolyOne Nymax™ GF 600 A 33 Natural Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
PolyOne Nymax™ GMF 604 40 UV Black 148 Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized
General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In..
Mold Temperature 48.9 - 82.2 °C
120 - 180 °F
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant
PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
Mold Temperature 48.9 - 76.7 °C
120 - 170 °F
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Mold Temperature 48.9 - 65.6 °C
120 - 150 °F
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Mold Temperature 49.0 - 93.0 °C
120 - 199 °F
PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated  (discontinued **)
Data provided by PolyOne.
Mold Temperature 48.9 - 60.0 °C
120 - 140 °F
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced
Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Mold Temperature 48.9 - 82.2 °C
120 - 180 °F
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Mold Temperature 48.9 - 98.9 °C
120 - 210 °F
PolyOne Lubri-Tech™ AT-15GM/15T Acetal-Copolymer, Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
PolyOne Lubri-Tech™ AT-15MCF/15T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated  (discontinued **)
Description/Features:Milled Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago
Mold Temperature 49.0 - 82.0 °C
120 - 180 °F
PolyOne Lubri-Tech™ NL-40GB/15T Nylon 6/12 - 40% Glass Bead Reinforced - 15% PTFE Lubricated  (discontinued **
Data provided by PolyOne.
Mold Temperature 48.9 - 76.7 °C
120 - 170 °F
Star Plastics ABS405 Extrusion Grade ABS
Information provided by Star Plastics, Inc.
Mold Temperature 48.9 - 76.7 °C
120 - 170 °F
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass
Information provided by Star Plastics, Inc.
Mold Temperature 48.9 - 76.7 °C
120 - 170 °F
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass
Information provided by Star Plastics, Inc.
Mold Temperature 48.9 - 65.6 °C
120 - 150 °F
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Mold Temperature 48.9 - 65.6 °C
120 - 150 °F
TPI Porene® ABS-KU650 Super High Heat ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Mold Temperature 48.9 - 60.0 °C
120 - 140 °F
Engineered Polymer Solutions ABS PCR 400, Recycled
General Purpose with 40% Post Consumer ABS. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions.
Mold Temperature 49.0 - 107 °C
120 - 225 °F
Average value: 89.5 °C Grade Count:14
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Mold Temperature 48.9 - 65.6 °C
120 - 150 °F
PolyOne Lubri-Tech™ AT-20GB/15T Acetal-Copolymer, Glass Bead Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 49.0 - 82.0 °C
120 - 180 °F
PolyOne Lubri-Tech™ AT-000/15T-2S Copolymer Acetal - 15% PTFE, 2% Silicone Lubricated  (discontinued **)
Data provided by PolyOne.
Mold Temperature 48.9 - 76.7 °C
120 - 170 °F
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded
Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc.
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
LTL Color Compounds ColorFast® GPA300 ABS
Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc.