| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
| Water Absorption | 5.0 % | 5.0 % | ISO 62 |
| Moisture Absorption | 1.50 % | 1.50 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 130 MPa | 18900 psi | conditioned; ISO 2039-1 |
| 230 MPa | 33400 psi | dry; ISO 2039-1 | |
| Tensile Strength at Break | 150 MPa | 21800 psi | conditioned; ISO 527-1/-2 |
| 200 MPa | 29000 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 3.5 % | 3.5 % | dry; ISO 527-1/-2 |
| 5.0 % | 5.0 % | conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 7.00 GPa | 1020 ksi | conditioned; ISO 527-1/-2 |
| 10.0 GPa | 1450 ksi | dry; ISO 527-1/-2 | |
| Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
| 9.50 J/cm² | 45.2 ft-lb/in² | conditioned; ISO 179/1eU | |
| 5.00 J/cm² @Temperature 30.0 °C |
23.8 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
| 5.50 J/cm² @Temperature 30.0 °C |
26.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
| 1.50 J/cm² | 7.14 ft-lb/in² | conditioned; ISO 179/1eA | |
| 0.900 J/cm² @Temperature 30.0 °C |
4.28 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 0.900 J/cm² @Temperature 30.0 °C |
4.28 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
| Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
| 200 °C | 392 °F | short term; EMS | |
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | ISO 75-1/-2 |
| Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
| 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | dry; IEC 60093 | |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
| Dielectric Strength | 35.0 kV/mm | 889 kV/in | conditioned; IEC 60243-1 |
| 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 | |
| Comparative Tracking Index | 550 V | 550 V | conditioned; IEC 60112 |
| 575 V | 575 V | dry; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Automotive | Automotive electr. and electronics, lighting | |
| Powertrain and Chassis | ||
| Electricals & Electronics | Electrical appliances | |
| Form | Granules | |
| Industry & Consumer goods | Heating systems | |
| Mechanical Engineering | ||
| Power transmission | ||
| Sports & Leisure | ||
| Tools & Accessories | ||
| Processing | Injection Molding |