| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit FRIANYL A63 TF10 Nylon 6.6 for injection molding, 10% PTFE lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit FRIANYL B63 KLZ Nylon 6 for injection molding Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit RECONYL B Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit FRIANYL A63 HS-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit FRIANYL B63 D Nylon 6., std. viscosity for injection molding Nylon 6., std. viscosity for injection molding, permanently flexible, developed for dowels.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit FRIANYL B63 E Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding (available only in nature).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit FRIANYL B63 EO Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, lubricated in surface.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit FRIANYL B63 HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit FRIANYL B63 M2 Nylon 6 for injection molding, 2% molybdenum disulphide lubricated Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Nilit RECONYL B F Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, highly crystallized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Ball Indentation Hardness | 130 - 170 MPa | 18900 - 24700 psi | Average value: 147 MPa Grade Count:7 |
| Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
| Ball Indentation Hardness | 130 - 310 MPa | 18900 - 45000 psi | Average value: 254 MPa Grade Count:23 |
| Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | cond.; ISO 2039-1 |
| Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
| Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Dry Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
| Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
| Schwartz Technical Plastics LAMINEX® 2140 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
| Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | conditioned; ISO 2039-1 |
| EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | dry; ISO 2039-1 |
| EMS-Grivory Grivory® BRZ 340 H PA6 Product description: Grilon BRZ 340 H is a heat stabilized, high viscosity, impact modified PA6 extrusion grade. Grilon BRZ 340 H has the following important properties:High impact strength at low t.. |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | 358 N; ISO 2039-1 |
| Azoty Tarnow™ TARNOFORM 300 LS POM Injection molding grade based on Tarnoform 300 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
| Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
| BASF Ultraform® H2320 004 POM Description: Is a POM, high-molecular-weight grade for extrusion of small thin-walled pipes and panel.Information provided by BASF |
|||
| Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
| BASF Ultraform® N2320 0035 LEV POM Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF |
|||
| Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
| BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
| Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
| BASF Ultraform® S2320 0035 POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF |
|||
| Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
| BASF Ultraform® N2320 0035 POM Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||