Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 35.0 kV/mm
889 kV/in
Covestro Apec® DP 1-9339/5 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba..
Dielectric Strength 35.0 kV/mm
889 kV/in
Covestro Apec® DP 1-9389 Polycarbonate  (discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and ha..
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243-1
DSM Akulon® K224-G3U (Dry) 15% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY
Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition..
Dielectric Strength 35.0 kV/mm
889 kV/in
K20/P20; IEC 60243-1
Styrolution Luran® S 757 G UV White 37019 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
Dielectric Strength 35.0 kV/mm
889 kV/in
K20/P20; IEC 60243-1
Styrolution Luran® S 778 Q42 Colored ASA
Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan..
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243
Teijin Panlite® G-3120PH For Cameras, Glass Fiber Reinforced Polycarbonate Resin
Reinforced with 30 % of special GF and improved appearance grade.Applications:Precision machinery, electric and electronic components that need dimensional accuracy and good appearance.Information p..
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY
Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu..
Dielectric Strength 35.0 kV/mm
889 kV/in
Under ambient atmosphere; ASTM D149
Unitika UNILATE® 1 SC PET
Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and ot..
Dielectric Strength 35.0 kV/mm
889 kV/in
No thickness given
ConocoPhillips Syncon® 32 Synthetic AW Hydraulic Fluid 32
Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommen..
Dielectric Strength 35.0 kV/mm

@Thickness 1.00 mm
889 kV/in

@Thickness 0.0394 in
IEC 60243-1
Covestro Apec® FR1892 High-Heat Polycarbonate
This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along..
Dielectric Strength 35.0 kV/mm
889 kV/in
Covestro Apec® HT KU 1-9343 High-Heat Polycarbonate, UV-Stabilized
Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243-1
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradegeneral purposecompared to FR 3000 improved chemical resistance and stress cracking behaviorVicat/B 120 temperature = 97 °CUL 94 V-0 at 1.5 mmPreprocessingMax. Water content
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243-1
DSM Akulon® K223-HGM24 Nylon 6-30% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243-1
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243-1
DSM Akulon® K224-G3 (Dry) 15% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Dielectric Strength 35.0 kV/mm
889 kV/in
dry; IEC 60243-1
DSM Akulon® K224-G8 PA6-GF40
40% Glass Reinforced
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243-1
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Dielectric Strength 35.0 kV/mm
889 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® B 70 GFE 15 H PA6-GF15
Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important prop..
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 243-1
CP-Polymer-Technik Wellamid® 6000 GS 40 HWCP 40% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 243-1
CP-Polymer-Technik Wellamid® 6000 GS 50 HWCP 50% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 243-1
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, UV Stabilized, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Dielectric Strength 35.0 kV/mm
889 kV/in
in transformer oil; IEC 60243-1
CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW
CENTRODAL GL has good dry running and emergency running properties. During the modification of POM + PE, a PE-UHMW is incorporated to the basic polyoxymethylene polymer. It leads to an improvement..
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60112
Proto3000 PC-ABS Fused Deposition Modeling Polymer
Description: PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior strength and heat resis..
Dielectric Strength 35.0 kV/mm
889 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40
Product description: Grivory HT1V-4 FWA natural is a 40 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
Dielectric Strength 35.0 kV/mm
889 kV/in
No thickness given
ConocoPhillips 32 Ultra-Clean Super Hydraulic Oil
Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1..
Dielectric Strength 35.0 kV/mm
889 kV/in
CEI 60243-1
Addiplast Addinyl B2 ZV40 Nylon 6, 40% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.