Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0070 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ASTM E831
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH  (d
AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4
DSM Akulon® S223-HPG8U (Dry) 43% Glass Reinforced, Impact Modified Nylon 66 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
Kuraray Genestarâ„¢ G1302 Nylon, 30% Glass Filled
Abrasion Resistance HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It delivers low..
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
LATI Latishield 38/11-08A G/10 ABS/PC, Steel/Glass Fiber Reinforced
EMI shielding product based on ABS/PC Blend (ABS/PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
LATI Latishield 66-10A H2 CETG/400 PA66, Steel/Glass Fiber Reinforced, Mineral Filled, Heat Stabilized
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI
LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0070 - 0.011 cm/cm
0.0070 - 0.011 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East)
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66
LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ASTM D955
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
b.o. ISO 2577
Covestro Makroblend® UT5207 PC/PBT Blend
Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Thickness 2.00 mm
0.0070 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4,2577
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Thickness 2.00 mm
0.0070 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® FU1007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® BG-40 S PA6-GF40
Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Thickness 4.00 mm
0.0070 in/in

@Thickness 0.157 in
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50
Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30
Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® TR 30 nat PA*
Product description: Grilamid TR 30 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 natural offers outstanding properties..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4 2577
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
Eurotec
Eurotec® Tecomid® NB30 GR15 BK005 FS90 PA6, 15% glass fiber reinforced, flame retardant - halogen & red phosphorus free, low smoke & toxic gas grade
Information provided by Eurotec®
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Conditioned, 50% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Conditioned, 50% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4 2577
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® TS V0 X PA666 FR
Product description: Grilon XE 5030 is a heat stabilized, flame retardant and self-extinguishing injection molding grade on the basis of PA6-PA66-alloy. Grilon XE 5030 features the following main pr..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ASTM D955
LNP Konduit® OTF-212-11 BK8-115 Polyphenylene Sulfide, Proprietary Filler  (discontinued **)
Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar..
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Lanxess Pocan® A 3131 000000 PBT+ASA, 30% glass fibers
PBT+ASA, 30% glass fibers, injection molding, low tendency to warp, improved surface finish
Copyright © lookpolymers.com All Rights Reserved