Polymer Property : Maximum Service Temperature, Air = 392 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Precision Polymer Engineering V60F Fluoroelastomer Compound
Peroxide/Litharge cured, Fluoroelastomer Rubber, 55-65 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line c..
Maximum Service Temperature, Air 200 °C
392 °F
Short Time; IEC 60216
PolyOne Bergamid™ A700 blue VN4817CF Polyamide 66 (Nylon 66)
Information provided by PolyOne
Maximum Service Temperature, Air 200 °C
392 °F
rated per UL card E54153
Arlon 515880R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate  (discontinued **)&l
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wr..
Maximum Service Temperature, Air 200 °C

@Time >=1200 sec
392 °F

@Time >=0.333 hour
Kazanorgsintez 271-274K Cable Composition Based on High Density Polyethylene
Production Method: Gaseous-phase method. Application: Compositions are intended for cover insulating lapping, protective covers and cables.Information Provided by Kazanorgsintez
Maximum Service Temperature, Air 200 °C
392 °F
short term
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing
Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG
Maximum Service Temperature, Air 200 °C
392 °F
Freudenberg Simrit V180 Non-Black Compound
Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p..
Maximum Service Temperature, Air 200 °C
392 °F
Momentive Performance Materials TSE3940 Flame Retardant Adhesive Sealant, Gray
TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater..
Maximum Service Temperature, Air 200 °C
392 °F
LATI Larton CE/60 PPS, 60% Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; ..
Maximum Service Temperature, Air 200 - 220 °C
392 - 428 °F
UL Temperature Rating
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations..
Maximum Service Temperature, Air 200 °C
392 °F
Silikony Polskie Silpasta P Silicone Paste
A consistency of hard VaselineTo improve thermal conduction in electrotechnical and mechanical devices.
Maximum Service Temperature, Air 200 °C
392 °F
Silikony Polskie Silpasta R Silicone Paste
Semi-liquid consistencyLubricant agent during assembly of PVC pipelines.
Maximum Service Temperature, Air 200 °C
392 °F
Short peaks operation
Polyram PlusTek PA320G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant
25% glass fiber reinforced, flame retardant and high stiffness polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Maximum Service Temperature, Air >= 200 °C
>= 392 °F
Short peaks operation
Polyram PlusTek PB320G6 Nylon 6, 30% Glass Fiber, Flame Retardant
30% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Maximum Service Temperature, Air 200 °C
392 °F
Short Term (3h)
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy
ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan..
Maximum Service Temperature, Air 200 °C
392 °F
Dow Corning MOLYKOTE® BG-20 SYNTHETIC BEARING GREASE
Polyol Ester grease especially for high speed bearingsFeatures: Lubricating bearings operating under a wide range of conditions, including high speeds, extreme temperatures and high loads. Handles ..
Maximum Service Temperature, Air 200 °C
392 °F
short term; EMS
EMS-Grivory Grivory® TSS/4 LF 2 PA666
Product description: Grilon TSS/4 LF 2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 2% lubricant (molybdenum disulphide). Grilon TSS/4 LF 2 has the following import..
Maximum Service Temperature, Air 200 °C
392 °F
Continuous use
Daikin NEOFLON NP-21 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion ..
Maximum Service Temperature, Air 200 °C
392 °F
Continuous
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy
Product Description: EPO TEK® H20E-LC is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also used exte..
Maximum Service Temperature, Air 200 °C
392 °F
ASTM D 3575
Eurofoam Siliconcell SIL 411 Silicone Foam Sheet
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.
Maximum Service Temperature, Air 200 °C
392 °F
per UL Card E54153
Arlon 0.010" (0.254 mm) Flexible Heater Silicone with Fiberglass Substrate (49586R010)
Cured silicone rubber with a minimum thickness of 0.0015 in. (0.038 mm)/ 0.0055 in. (0.14 mm) Prime Coated 1681 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.003 in. (0.08 mm); 0...
Maximum Service Temperature, Air 200 °C
392 °F
rated per UL card E54153
Arlon 32580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s..
Maximum Service Temperature, Air 200 °C
392 °F
rated per UL card E54153
Arlon 30580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The d..
Maximum Service Temperature, Air 200 °C
392 °F
rated per UL card E54153
Arlon 49581XC010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Gray gum on glass fiber fabricThis data Represents typical values for the production material. The data ..
Maximum Service Temperature, Air 200 °C
392 °F
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned)
Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF
Maximum Service Temperature, Air 200 °C
392 °F
Long Term
CENTROPLAST CENTROTRON Polyphenylene sulfide
CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used at high operating temperatures. Applications include plug connectors, sensor housings and parts for electrica..