Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 130 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
Nilit FRIANYL A63 TF10 Nylon 6.6 for injection molding, 10% PTFE lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
Nilit FRIANYL A63 TF20 Nylon 6.6 for injection molding, 20% PTFE lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
Nilit FRIANYL B63 E Raw extruded nylon 6 for injection molding
Raw extruded nylon 6 for injection molding (available only in nature).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
Nilit FRIANYL B63 EO Raw extruded nylon 6 for injection molding
Raw extruded nylon 6 for injection molding, lubricated in surface.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
Nilit FRIANYL B63 HS-KV20 Nylon 6 for injection molding, 20% glass ball reinforced
Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
Nilit FRIANYL B63 M2 Nylon 6 for injection molding, 2% molybdenum disulphide lubricated
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
Nilit RECONYL B F Recycled nylon 6 for injection molding
Recycled nylon 6 for injection molding, highly crystallized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 130 - 170 MPa
18900 - 24700 psi
Average value: 147 MPa Grade Count:7
Overview of materials for Phenolic, Novolac, Fabric Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values ..
Ball Indentation Hardness 130 - 310 MPa
18900 - 45000 psi
Average value: 195 MPa Grade Count:8
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Ball Indentation Hardness 130 MPa
18900 psi
Conditioned; ISO 2039-1
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
Ball Indentation Hardness 130 MPa
18900 psi
Hc 30; ISO 2039; partially
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated
Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH
Ball Indentation Hardness 130 MPa
18900 psi
Hc 30; ISO 2039; partially
Schwartz Technical Plastics LAMINEX® 2100 Cotton Fabric, Phenolic Resin Impregnated
Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH
Ball Indentation Hardness 130 MPa
18900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® AG-30 PA66-GF30
Information provided by EMS Grivory
Ball Indentation Hardness 130 MPa
18900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BG-40 HM PA6-GF40
Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop..
Ball Indentation Hardness 130 MPa
18900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSG-30/4 V0 PA666-GF30 FR
Product description: Grilon TSG-30/4 V0 is a heat stabilized, flame retardant, self-extinguishing engineering thermoplastic, reinforced with glass-fiber 30% (by weight) based on a semi-crystalline P..
Ball Indentation Hardness 130 MPa
18900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® LC-3H black PA12-CF30
Product description: Grilamid LC-3H BLACK is a Polyamide 12 injection molding product reinforced with 30 % carbon fibers. The product is inherently black and is only available in this color.Main Att..
Ball Indentation Hardness 130 MPa
18900 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 300 LS POM
Injection molding grade based on Tarnoform 300 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
BASF Ultradur B 2550 PBT
Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in..
Ball Indentation Hardness 130 MPa

@Load 36.5 kg,
Time 30.0 sec
18900 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® H2320 004 POM
Description: Is a POM, high-molecular-weight grade for extrusion of small thin-walled pipes and panel.Information provided by BASF
Ball Indentation Hardness 130 MPa

@Load 36.5 kg,
Time 30.0 sec
18900 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® N2320 0035 LEV POM
Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF
Ball Indentation Hardness 130 MPa

@Load 36.5 kg,
Time 30.0 sec
18900 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® S2320 0035 LEV POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF
Ball Indentation Hardness 130 MPa
18900 psi
value at 30 sec.; ISO 2039-1
CENTROPLAST CENTROPHEN GF Polyphenylene ether 30% glass fiber
This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include electronic housings, valve pistons, and support rollers.Inform..
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
BASF Ultradur B 4500 PBT
Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660.
Ball Indentation Hardness 130 MPa

@Load 36.5 kg,
Time 30.0 sec
18900 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® W2320 0035 POM
Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039-1
BASF Ultradur B 6550 PBT
Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes.
Ball Indentation Hardness 130 MPa
18900 psi
ISO 2039
GEHR Plastics PPE-30GF Polyphenylene Ether, 30% Glass Fiber  (discontinued **)
The 30% glass fiber reinforced PPE has an improved dimensional stability, a very high stiffness and heat resistance that allows further uses.
Copyright © lookpolymers.com All Rights Reserved