| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
| PolyOne OnFlex™ S HF 50A-3S1981 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
| Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
| Nilit FRIANYL A63 GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
| Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
| Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
| Nilit FRIANYL A63 W-GV30 Nylon 6.6, std. viscosity for injection molding, 30% glass fiber reinforced Nylon 6.6, std. viscosity for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
| Nilit FRIANYL B63 L-HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Comparative Tracking Index | 550 V | 550 V | |
| Radici Radiflam® A RV300AF (cond.) Nylon 66-30GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
| Comparative Tracking Index | 550 V | 550 V | |
| Radici Radilon® A ERV1906LK (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
| Comparative Tracking Index | 550 V | 550 V | |
| Radici Radilon® S RV300R (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
| Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
| Nilit FRIANYL B63 HS-GV40 Nylon 6 for injection molding, 40% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
| Nilit FRIANYL C73 GV15 Nylon 6.6/6 for injection molding, 15% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Comparative Tracking Index | 550 V | 550 V | |
| Radici Radilon® S RCP3010LK (cond.) Nylon 6 PA6 30% Glass Fiber and mineral filler reinforced injection molding grade. Good stiffness and good dimensional stability. Heat stabilized, good surface finish.Information provided by Radici group. |
|||
| Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
| DSM Akulon® K224-HG5 Nylon 6-25% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
| Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 596 V Grade Count:14 |
| Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
| Comparative Tracking Index | 550 V | 550 V | Solution A, Rating; IEC 60112 |
| Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties |
|||
| Comparative Tracking Index | 550 V | 550 V | UL 746 |
| Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
| Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
| Ter Hell Plastic Terez® PA 6 7750 TK Polyamide 6 Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information pr.. |
|||
| Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
| CP-Polymer-Technik Wellamid® 6000 GV 20 HWCP 20% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
| Comparative Tracking Index | 550 V | 550 V | conditioned; IEC 60112 |
| EMS-Grivory Grivory® TSGZ-50 PA666-GF50 Information provided by EMS Grivory |
|||
| Comparative Tracking Index | 550 V | 550 V | DAM; IEC 60112 |
| DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
| Comparative Tracking Index | 550 V | 550 V | Test solution A; IEC 60112 |
| BASF Ultramid® B3ZG3 BK 30564 15% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 15% glass fiber reinforced injection-molding grade, for instance, for automotive cable conduits.Information provided by BASF |
|||
| Comparative Tracking Index | 550 V | 550 V | Test solution A; IEC 60112 |
| BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Dry) Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire .. |
|||
| Comparative Tracking Index | 550 V | 550 V | Test Solution A; IEC 60112 |
| Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
| Comparative Tracking Index | 550 V | 550 V | Test Solution A; IEC 60112 |
| BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
| Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
| BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned) Ultramid A 3HG2 is a 10% glass fiber reinforced grade of nylon 6/6 for injection molding. |
|||
| Comparative Tracking Index | 550 V | 550 V | |
| Plastcom SLOVASTER® B2 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
| Comparative Tracking Index | 550 V | 550 V | |
| Radici Radilon® S CV300 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
| Comparative Tracking Index | 550 V | 550 V | Test Solution A; IEC 60112 |
| BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry) Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo.. |
|||
| Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |
| Addiplast Addinyl B2 V15 Nylon 6, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||