| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled |
| Manufacturer | Addiplast |
| Trade Name | Addinyl |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Addiplast Addinyl A2 ZP40 Nylon 66, 40% Mineral Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 85 | 85 | Conditioned; ISO 868 |
| 88 | 88 | ISO 868 | |
| Tensile Strength at Break | 60.0 MPa | 8700 psi | Conditioned; ISO R 527 |
| 85.0 MPa | 12300 psi | ISO R 527 | |
| Elongation at Yield | 10 % | 10 % | ISO R 527 |
| 35 % | 35 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 1.60 GPa | 232 ksi | Conditioned; ISO 178 |
| 5.10 GPa | 740 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180/1A |
| 9.00 kJ/m² | 4.28 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | NB | NB | ISO 179/IeU |
| NB | NB | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/IeA |
| 0.900 J/cm² | 4.28 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 55.0 µm/m-°C | 30.6 µin/in-°F | ASTM E831 |
| Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Dielectric Strength | 25.0 kV/mm | 635 kV/in | Conditioned; CEI 60243-1 |
| 30.0 kV/mm | 762 kV/in | CEI 60243-1 | |
| Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |