| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics EXTEM UH1016 TPI Blend
High heat amorphous TPI Blend, Chemical Resistant, High Flow
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER
LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a..
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Asia Pacific)
Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm ..
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS
LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | DIN 53453/ISO 179 |
|
Ineos Nova S-6600MG Compact Polystyrene Microgranulates
(discontinued **)
High impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm especially useful for compounding and extrusion applications. Due to the higher viscosity intensive mixing with thermoplas..
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER
Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East)
Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only.
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | Notch A; ISO 180 |
|
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East)
VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings.
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East)
VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets.
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East)
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON RX04031 PA 66 (Europe-Africa-Middle East)
LNP* STARFLAM* RX04031 is a compound based on PA66 resin containing Carbon Fiber, Glass Fiber, Flame Retardant. Added features include: Non-Brominated & Non-Chlorinated Flame Retardant, Electricall..
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature 23.0 °C
|
4.28
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermocomp EF008EXP PEI (Europe-Africa-Middle East)
LNP* Thermocomp* EF008EXP is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SABIC-IP ..
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature 23.0 °C
|
4.28
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermocomp LC008 PEEK (Europe-Africa-Middle East)
LNP* Thermocomp* LC008 is a compound based on Polyetheretherketone resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA
LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare.
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180 |
|
Tisan TISLAMID® 6 20% Glass Fiber Reinforced, Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180-93 |
|
Wellman Wellamid® GFT1699-WBK1 13% Glass Fiber Reinforced, Weatherable Black Nylon 66
Description: Glass Fiber Reinforced, Weatherable Black Nylon 66Information provided by Wellman.
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature -40.0 °C
|
4.28
ft-lb/in² <br>@Temperature -40.0 °F
|
Brittle break; ISO 180 |
|
DSM Fibre Intermediates Nyrim® 1500 (Dry)
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec..
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature -40.0 °C
|
4.28
ft-lb/in² <br>@Temperature -40.0 °F
|
Brittle break; ISO 180 |
|
DSM Fibre Intermediates Nyrim® 2000 (Dry)
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec..
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature -40.0 °C
|
4.28
ft-lb/in² <br>@Temperature -40.0 °F
|
ISO 180/1A |
|
DuPont Performance Polymers Delrin® 500T BK602 Acetal (POM)
(Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T BK602 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180/1A |
|
Addiplast Addilene J 520 T30 Polypropylene Copolymer
Mineral reinforced, improved rigidityInformation provided by Addiplast.
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ASTM D256 |
|
Beijing Ranger Chem PBT-201-G25 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature -20.0 °C
|
4.28
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polyplastic Armlen® PP 12IM-895 Impact Modified Polypropylene
Impact modified polypropylene composite materialUV resistantInformation provided by PolyPlastic Group.
|
|||
| Izod Impact, Notched (ISO) |
9.00
kJ/m² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180 |
|
LNP Thermocomp® UF-1008 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
|
|||
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC
LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated.
|
|||