Material Notes:
PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump housings, pump impellers and water meter components.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Moisture Absorption 0.0400 %
0.0400 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.10 %
0.10 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0040 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 3.2 g/10 min

@Load 5.00 kg,
Temperature 280 °C
3.2 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
Melt Index of Compound 2.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
50 mm/min; ISO 527
130 MPa
18900 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
50 mm/min; ISO 527
3.0 %
3.0 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 8.20 GPa
1190 ksi
1 mm/min; ISO 527
8.60 GPa
1250 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 160 MPa
23200 psi
1.3 mm/min, 50 mm span; ASTM D790
160 MPa
23200 psi
2 mm/min; ISO 178
Flexural Modulus 6.80 GPa
986 ksi
2 mm/min; ISO 178
7.20 GPa
1040 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 5.90 J/cm
11.1 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 20.0 J

@Temperature 23.0 °C
14.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
75.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 147 °C

@Thickness 3.20 mm
297 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 139 °C
282 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
139 °C

@Thickness 3.20 mm
282 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 147 °C
297 °F
Rate B/50; ASTM D1525
147 °C
297 °F
Rate B/50; ISO 306
149 °C
300 °F
Rate B/120; ISO 306