| UBE 1022C2 NCH Nylon 6 Film |
Nylon 6, Film Grade |
|
| UBE 1022FDX23 Nylon 6 Homopolymer Film |
Nylon 6, Film Grade |
|
| UBE 1022FDX29 Nylon 6 Homopolymer Film |
Nylon 6, Film Grade |
|
| UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=4.5) |
Nylon 6 Fiber |
|
| UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=5) |
Nylon 6 Fiber |
|
| UBE 1022T Nylon 6 Monofilament (Drawing Ratio=4.5) |
Nylon 6 Fiber |
|
| UBE 1022T Nylon 6 Monofilament (Drawing Ratio=4.8) |
Nylon 6 Fiber |
|
| UBE 1022T Nylon 6 Monofilament (Drawing Ratio=5) |
Nylon 6 Fiber |
|
| UBE 1024FD-1 Nylon 6 Film |
Nylon 6, Film Grade |
|
| UBE 1024FDX41 Nylon 6 BOPA Film |
Nylon 6, Film Grade |
|
| UBE 1026B1 Nylon 6 Homopolymer Film |
Nylon 6, Film Grade |
|
| UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=4.5) |
Nylon 6/66 |
|
| UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=4.8) |
Nylon 6/66 |
|
| UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=5) |
Nylon 6/66 |
|
| UBE 5033B Air Blown Nylon 6/66 Film |
Film |
|
| UBE 5033B Nylon 6/66 Film |
Film |
|
| UBE 5033FDX27 Air Blown Nylon 6/66 Film |
Film |
|
| UBE 5033T Nylon 6/66 Monofilament (Drawing Ratio=5) |
Nylon 6/66 |
|
| UBE 5033T Nylon 6/66 Monofilament (Drawing Ratio=5.5) |
Nylon 6/66 |
|
| UBE 5034C2 NCH Nylon 6/66 Film |
Film |
|
| UBE 5034FDX17 Air Blown Nylon 6/66 Film |
Film |
|
| UBE 5034FDX33 Air Blown Nylon 6/66 Film |
Film |
|
| UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=4.5) |
Nylon 6/66 |
|
| UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=5.5) |
Nylon 6/66 |
|
| UBE 5034MTAX1 Nylon 6/66 Monofilament (Drawing Ratio=4.5) |
Nylon 6/66 |
|
| UBE 5034MTAX1 Nylon 6/66 Monofilament (Drawing Ratio=5) |
Nylon 6/66 |
|
| UBE 5034MTAX1 Nylon 6/66 Monofilament (Drawing Ratio=5.5) |
Nylon 6/66 |
|
| UBE 5034MTAX1 Nylon 6/66 Monofilament (Drawing Ratio=6) |
Nylon 6/66 |
|
| UBE 5034T Nylon 6/66 Monofilament (Drawing Ratio=4.5) |
Nylon 6/66 |
|
| UBE 5034T Nylon 6/66 Monofilament (Drawing Ratio=5) |
Nylon 6/66 |
|
| UBE 7024B Nylon 6/12 Copolymer Film |
Nylon 612, Unreinforced |
|
| UBE 7024B Nylon 6/12 Film |
Nylon 612, Unreinforced |
|
| UBE 7034B Nylon 6/12 Copolymer Film |
Nylon 612, Unreinforced |
|
| UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=5) |
Nylon 612 |
|
| UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=5.5) |
Nylon 612 |
|
| UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=6) |
Nylon 612 |
|
| UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5, Diameter 0.4 mm) |
Nylon 612 |
|
| UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5, Diameter 2 mm) |
Nylon 612 |
|
| UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5.5, Diameter 0.4 mm) |
Nylon 612 |
|
| UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5.5, Diameter 2 mm) |
Nylon 612 |
|
| UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=6, Diameter 0.4 mm) |
Nylon 612 |
|
| UBE 7128B Nylon 6/12 Copolymer |
Nylon 612, Impact Modified |
|
| UBE A (High-Cis) HIPS (n-DM =0.03 wt %) |
Polystyrene, Impact Modified |
|
| UBE B (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) |
Polystyrene, Impact Modified |
|
| UBE B128 Polyethylene |
Polyethylene (PE) |
|
| UBE C (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) |
Polystyrene, Impact Modified |
|
| UBE F022 Polyethylene |
Polyethylene (PE) |
|
| UBE F022NH Polyethylene |
Polyethylene (PE) |
|
| UBE F022SE Polyethylene |
Polyethylene (PE) |
|
| UBE F023 Polyethylene |
Polyethylene (PE) |
|
| UBE F120N Polyethylene |
Polyethylene (PE) |
|
| UBE F222 Polyethylene |
Polyethylene (PE) |
|
| UBE F222NH Polyethylene |
Polyethylene (PE) |
|
| UBE F320 Polyethylene |
Polyethylene (PE) |
|
| UBE F522 Polyethylene |
Polyethylene (PE) |
|
| UBE F522N Polyethylene |
Polyethylene (PE) |
|
| UBE J1019 Polyethylene |
Polyethylene (PE) |
|
| UBE J2522 Polyethylene |
Polyethylene (PE) |
|
| UBE J3519 Polyethylene |
Polyethylene (PE) |
|
| UBE L719 Polyethylene |
Polyethylene (PE) |
|
| UBE P7115U Electronic Grade Nylon Copolymer Powder |
Nylon 612 |
|
| UBE PAE1200U Nylon Elastomer |
Nylon |
|
| UBE PAE1200U2 Electronic Grade Nylon Elastomer |
Nylon |
|
| UBE R300 Polyethylene |
Polyethylene (PE) |
|
| UBE R500 Polyethylene |
Polyethylene (PE) |
|
| UBE UBEPOL B -B HIPS (Low-cis) |
Polystyrene, Impact Modified |
UBEPOL
|
| UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber (Raw Polymer) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR13HB HIPS (n-DM =0.03 wt %) |
Polystyrene, Impact Modified |
UBEPOL
|
| UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber (Raw Polymer) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR150 Synthetic Rubber (Compound) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber (Raw Polymer) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR150B Synthetic Rubber (Compound) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber (Raw Polymer) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR150L Synthetic Rubber (Compound) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR15H HIPS (n-DM =0.03 wt %) |
Polystyrene, Impact Modified |
UBEPOL
|
| UBE UBEPOL BR15HB HIPS (n-DM =0.03 wt %) |
Polystyrene, Impact Modified |
UBEPOL
|
| UBE UBEPOL BR15HL HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) |
Polystyrene, Impact Modified |
UBEPOL
|
| UBE UBEPOL BR15HL HIPS (n-DM =0.03 wt %) |
Polystyrene, Impact Modified |
UBEPOL
|
| UBE UBEPOL BR230 Non-Oil Extended Synthetic Rubber (Raw Polymer) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber (Raw Polymer) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR34HL HIPS (stirring rate = 400 rpm) |
Polystyrene, Impact Modified |
UBEPOL
|
| UBE UBEPOL BR34HL HIPS (stirring rate = 500 rpm) |
Polystyrene, Impact Modified |
UBEPOL
|
| UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber (Raw Polymer) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL VCR303 Synthetic Rubber (Raw Polymer) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|
| UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) |
Rubber or Thermoset Elastomer (TSE) |
UBEPOL
|