UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber (Raw Polymer)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer UBE
Trade Name UBEPOL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber (Raw Polymer).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Microstructure: cis: 98trans: 1vinyl: 1Information provided by UBE.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D1505
Volatiles 0.30 %
0.30 %
ASTM D1416
Viscosity 65 cP

@Temperature 25.0 °C
65 cP

@Temperature 77.0 °F
Solution Viscosity in 5 wt.% Toluene; UBE Method
Viscosity Measurement 2.0

@Temperature 30.0 °C
2.0

@Temperature 86.0 °F
Intrinsic Viscosity in Toluene; UBE Method
Mooney Viscosity 34

@Temperature 100 °C
34

@Temperature 212 °F
ML1+4; ASTM D1646
Molecular Weight 510000 g/mol
510000 g/mol
No units specified (Number Average Molecular Weight (10^4) = 21); UBE Method
Ash 0.050 %
0.050 %
ASTM D1416