Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical properties including transparency and glossiness, and making the material ideal for further processing.Transparency:Superior transparency and glossiness even for applications involving processing of thick objects.Ease of Processing: Excellent fluidity and melt tension characteristics suited to a wide range of molding methods.Inflation molding - can be molded into even thick or wide products with superior bubble stability.Extrusion lamination - can be drawn down even at high speed.Blow molding - can be molded producing a very smooth surface.Injection molding - can be molded even into very thin products.Strength: Good balance in length and breadth with superior tearing strength lengthways.Application: Injection moldingFeatures: Moldability GlossinessInformation provided by UBE.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ASTM D2240
Tensile Strength at Break 9.50 MPa
1380 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Strength 13.0 MPa
1890 psi
Olsen; ASTM D747
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Brittleness Temperature -42.0 °C
-43.6 °F
ASTM D746