| Category | Polymer , Film , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Film Grade |
| Manufacturer | UBE |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | UBE 1024FDX41 Nylon 6 BOPA Film.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Oxygen Transmission Rate | 53.0 - 54.0 cc/m²/day | 3.41 - 3.48 cc/100 in²/day | ASTM D-3985 |
| Relative Viscosity | 3.38 - 3.5 cP | 3.38 - 3.5 cP | 96% H2SO4 |
| 3.61 - 3.75 cP | 3.61 - 3.75 cP | 98% H2SO4 | |
| Thickness | 13.0 - 15.0 microns | 0.512 - 0.591 mil | Gauge |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Elongation at Break, MD | 120 % | 120 % | ASTM D-882 |
| Film Elongation at Break, TD | 130 % | 130 % | ASTM D-882 |
| Secant Modulus, MD | 1.25 GPa | 181 ksi | ASTM D-882 |
| Secant Modulus, TD | 1.30 GPa | 189 ksi | ASTM D-882 |
| Coefficient of Friction, Dynamic | 0.37 | 0.37 | non treated surface; ASTM D-1894 |
| Coefficient of Friction, Static | 0.37 | 0.37 | (non treated surface); ASTM D-1894 |
| Film Tensile Strength at Break, MD | 224 MPa | 32500 psi | ASTM D-882 |
| Film Tensile Strength at Break, TD | 213 MPa | 30900 psi | ASTM D-882 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 215 - 225 °C | 419 - 437 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 3.0 % | 3.0 % | ASTM D-1003 |
| Gloss | 146 % | 146 % | ASTM D-523 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 200 - 220 °C | 392 - 428 °F | C1 |
| 210 - 230 °C | 410 - 446 °F | C2 | |
| 230 - 240 °C | 446 - 464 °F | C3 | |
| 240 - 250 °C | 464 - 482 °F | C4 | |
| 250 - 260 °C | 482 - 500 °F | AD | |
| 250 - 260 °C | 482 - 500 °F | CF | |
| 250 - 260 °C | 482 - 500 °F | D1- D4 |