UBE P7115U Electronic Grade Nylon Copolymer Powder

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer UBE
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE P7115U Electronic Grade Nylon Copolymer Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication Systems through the world.Comments: nylon 6/12 copolymerInformation provided by UBE.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Melt Flow 60 g/10 min

@Load 1.00 kg,
Temperature 190 °C
60 g/10 min

@Load 2.20 lb,
Temperature 374 °F
ASTM D1238R
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
ASTM D2240
Tensile Strength at Break >= 27.0 MPa
>= 3920 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Strength 23.0 MPa
3340 psi
ASTM D790
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 145 °C
293 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 46.0 °C
115 °F
ASTM D648