Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE 5034MTAX1 Nylon 6/66 Monofilament (Drawing Ratio=5)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer UBE
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE 5034MTAX1 Nylon 6/66 Monofilament (Drawing Ratio=5).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Specialties: Excellent transparency and softness, Specially developed for very big size diameter (over 2mm in diameter)Applications: Big size diameter and high transparency required applications (over 2 mm diameter is suitable, like a main line of long line and etc.)Information provided by UBE.
Mechanical Properties Metric English Comments
Elongation at Break 39 %
39 %
Knot Elongation
50 %
50 %
Line Elongation
Tenacity 0.282 N/tex
3.20 g/denier
Knot Strength
0.415 N/tex
4.70 g/denier
Line Strength
0.786 N/tex
8.90 g/denier
Tensile Modulus
Descriptive Properties Value Comments
Appearance Very Clear & Glossy