| Category | Polymer , Film , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Film Grade |
| Manufacturer | UBE |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | UBE 1022FDX29 Nylon 6 Homopolymer Film.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Relative Viscosity | 3.31 - 3.43 cP | 3.31 - 3.43 cP | 96% H2SO4 |
| 3.53 - 3.67 cP | 3.53 - 3.67 cP | 98% H2SO4 | |
| Thickness | 40.0 microns | 1.57 mil |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Elongation at Break, MD | 440 % | 440 % | |
| Secant Modulus, MD | 0.470 GPa | 68.2 ksi | |
| Coefficient of Friction, Dynamic | 0.30 | 0.30 | 20 deg. C 55% RH |
| Coefficient of Friction, Static | 0.46 | 0.46 | ( 20 deg. C 55% RH ) |
| Film Tensile Strength at Break, MD | 95.0 MPa | 13800 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 215 - 225 °C | 419 - 437 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 3.2 % | 3.2 % | |
| Gloss | 135 % | 135 % |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 200 - 220 °C | 392 - 428 °F | C1 |
| 210 - 230 °C | 410 - 446 °F | C2 | |
| 230 - 240 °C | 446 - 464 °F | C3 | |
| 240 - 250 °C | 464 - 482 °F | C4 | |
| 250 - 260 °C | 482 - 500 °F | AD | |
| 250 - 260 °C | 482 - 500 °F | CF | |
| 250 - 260 °C | 482 - 500 °F | D1- D4 | |
| Roll Temperature | 80.0 °C | 176 °F | Chill Roll Temperature |