Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Clariant > Category : Nylon 66 Product List

Tips:100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category Trade Name
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Nylon 66
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Nylon 66, Heat Stabilized
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated Nylon 66, 20% Glass Fiber Filled
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated Nylon 66, 40% Glass Fiber Filled
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Nylon 66
Clariant PA123G20 Nylon 66, 20% Glass Fiber, Impact Modified, Heat Stabilized Nylon 66, 20% Glass Fiber Filled
Clariant PA123G25 Nylon 66, 25% Glass Fiber, Impact Modified, Heat Stabilized Nylon 66, Heat Stabilized
Clariant PA123G30 Nylon 66, 30% Glass Fiber, Impact Modified, Heat Stabilized Nylon 66, Heat Stabilized
Clariant PA131 Nylon 66, Highly Impact Modified Nylon 66, Impact Grade
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Nylon 66
Clariant Renol 6601FR Nylon 66, Flame Retardant Nylon 66, Unreinforced, Flame Retardant
Clariant Renol 66G15BL-195 Blue Nylon 66, 15% Glass Fiber Reinforced Nylon 66, 20% Glass Fiber Filled
Clariant Renol 66G33 2% Moly Nylon 66, 33% Glass Fiber Reinforced, 2% Molybdenum Disulfide Lubricated Nylon 66, MoS2 Filled
Clariant Renol 66G33HSL Nylon 66, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated Nylon 66, 30% Glass Fiber Filled
Clariant Renol BR2025 Nylon 66, Impact Modified Nylon 66, Impact Grade
Clariant Renol BR2029 Nylon 66, General Purpose, Black Nylon 66
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced Nylon 66, Glass/Mineral Filled
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated Nylon 66, PTFE Filled
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Nylon 66
Clariant Renol PA101L Nylon 66, General Purpose, Lubricated Nylon 66
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated Nylon 66
Clariant Renol PA111 Nylon 66, General Purpose Nylon 66
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled Nylon 66, Glass/Carbon Fiber Filled
Clariant Renol PA111G35IF Nylon 66, 35% Glass Fiber, Improved Flow Nylon 66, 40% Glass Fiber Filled
Clariant Renol PA111G50 Nylon 66, 50% Glass Fiber Nylon 66, 50% Glass Fiber Filled
Clariant Renol PA111G50IF Nylon 66, 50% Glass Fiber, Improved Flow Nylon 66, 50% Glass Fiber Filled
Clariant Renol PA111G60 Nylon 66, 60% Glass Fiber Nylon 66, 60% Glass Fiber Filled
Clariant Renol PA112 Nylon 66, Nucleated Nylon 66, Nucleated
Clariant Renol PA113 Nylon 66, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol PA113C Nylon 66, Molybdenum Disulfide Lubricated Nylon 66, MoS2 Filled
Clariant Renol PA113G13 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated Nylon 66, 10% Glass Fiber Filled
Clariant Renol PA113G13X050 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Improved Ductility Nylon 66, 10% Glass Fiber Filled
Clariant Renol PA113G15 Nylon 66, 15% Glass Fiber Nylon 66, 20% Glass Fiber Filled
Clariant Renol PA113G33HR Nylon 66, 33% Glass Fiber, Heat Stabilized, Hydrolysis Resistant Nylon 66, Heat Stabilized
Clariant Renol PA11BK FDA Nylon 66, General Purpose, FDA, Black Nylon 66
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Nylon 66, 10% Glass Fiber Filled
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Nylon 66, 30% Glass Fiber Filled
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol PA1SP0003 Nylon 66, PE Modified Nylon 66
Clariant Renol PA1SP0004 Nylon 66, High Impact Modified, ESD Nylon 66, Impact Grade
Clariant Renol PA1SP0005 Nylon 66, Impact Modified, Glass Reinforced Nylon 66, Glass Reinforced, Impact Grade
Clariant Renol PA1SP0019 Nylon 66/PPS Alloy, 20% Glass, 20% Mineral Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Clariant Renol PA211 Nylon 6, General Purpose Nylon 66, Heat Stabilized
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy Nylon 66, 10% Glass Fiber Filled
Clariant Renol 6601L Nylon 66, Lubricated Nylon 66
Clariant Renol 6601M Nylon 66, Molybdenum Disulfide Lubricated Nylon 66, MoS2 Filled
Clariant Renol 6602-L Nylon 66, Internally Lubricated Nylon 66
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol 6608G33HSL Nylon 66, 33% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol 6608G43 Nylon 66, 43% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Nylon 66, 40% Glass Fiber Filled
Clariant Renol 6608-L Nylon 66, High Impact Modified, Lubricated Nylon 66, Impact Grade
Clariant Renol 6608-L UV Black Nylon 66, High Impact Modified, Lubricated, UV Stable Nylon 66, Impact Grade
Clariant Renol 6608-LLT Nylon 66, High Impact Modified, Lubricated, Low Temp Impact Nylon 66, Impact Grade
Clariant Renol 6622-L Nylon 66, Glass Fiber Filled, Lubricated Nylon 66, Glass Reinforced, Impact Grade
Clariant Renol 6642 2% Moly Nylon 66, Extrusion Grade, 2% Molybdenum Disulfide Lubricated Nylon 66, MoS2 Filled
Clariant Renol 66B40 Nylon 66, 40% Glass Bead Filled Nylon 66, Glass Bead Filled
Clariant Renol PA111BK S&P Nylon 66, General Purpose Nylon 66
Clariant Renol PA111G33 Nylon 66, 33% Glass Fiber Nylon 66, 30% Glass Fiber Filled
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated Nylon 66, Heat Stabilized
Clariant Renol PA121 Nylon 66, Impact Modified Nylon 66, Impact Grade
Clariant Renol 66G33-L Nylon 66, 33% Glass Fiber Reinforced, Lubricated Nylon 66, 30% Glass Fiber Filled
Clariant Renol PA111G30IF Nylon 66, 30% Glass Fiber, Improved Flow Nylon 66, 30% Glass Fiber Filled
Copyright © lookpolymers.com All Rights Reserved