| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
| Elongation at Break | 75 % | 75 % | ASTM D638 |
| Flexural Yield Strength | 110 MPa | 16000 psi | ASTM D790 |
| Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm <br>@Temperature 22.8 °C |
1.00 ft-lb/in <br>@Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 175 °C | 347 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
| Mold Temperature | 65.6 - 79.4 °C | 150 - 175 °F | |
| Dry Time | 2 - 4 hour <br>@Temperature 79.4 °C |
2 - 4 hour <br>@Temperature 175 °F |
to ensure moisture content is less than 0.2% |
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
| 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial | |
| Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
| Shot Size | 30 - 80 % | 30 - 80 % | |
| Screw Speed | 20 - 100 rpm | 20 - 100 rpm |