Arlon 10172R080 0.080" (2.3 mm) Cured Silicone Rubber Vacuum Bag |
Silicone Rubber |
|
Arlon 10292R062 Cured Silicone Rubber (Unsupported) with Polyethylene Liner |
Silicone Rubber |
|
Arlon 10322B050 0.050" (1.27 mm) Fully Cured Silicone Rubber with Polyethylene Liner |
Silicone Rubber |
|
Arlon 10502N060 0.060" (1.52 mm) Cured/Post-Cured Unsupported Silicone Rubber |
Silicone Rubber |
|
Arlon 10502R010 0.010" (.254 mm) Cured/Post-Cured Unsupported Silicone Rubber |
Silicone Rubber |
|
Arlon 10502R020 0.020" (0.508 mm) Cured Silicone Rubber (Unsupported) |
Silicone Rubber |
|
Arlon 10502R030 0.040" (1.02 mm) Cured/Post-Cured Unsupported Silicone Rubber |
Silicone Rubber |
|
Arlon 10502R125 Cured/Post-cured, Unsupported Silicone Rubber |
Silicone Rubber |
|
Arlon 10842N125 Cured/Post-cured, Unsupported Silicone Rubber |
Silicone Rubber |
|
Arlon 10842R125 Cured/Post-cured, Unsupported Silicone Rubber |
Silicone Rubber |
|
Arlon 10842S018 0.018" (0.457 mm) Fully Cured, Unsupported, Silicone Rubber |
Silicone Rubber |
|
Arlon 10842S020 0.020" (0.508 mm) Fully Cured, Unsupported, Silicone Rubber |
Silicone Rubber |
|
Arlon 10842S060 0.060" (1.52 mm) Fully Cured, Unsupported, Silicone Rubber |
Silicone Rubber |
|
Arlon 10842S085 Fully Cured, Unsupported Silicone Rubber |
Silicone Rubber |
|
Arlon 10842S090 Fully Cured, Unsupported Silicone Rubber |
Silicone Rubber |
|
Arlon 10842S125 Cured/Post-cured, Unsupported Silicone Rubber |
Silicone Rubber |
|
Arlon 15370P020 0.020" (0.508 mm) Uncured Silicone Rubber on a Mylar Carrier |
Silicone Rubber |
|
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier |
Silicone Rubber |
|
Arlon 18146R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 18596R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 18646B026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 18976XA023 Silicone Rubber/Fiberglass Laminate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19146R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19220R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19540R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19562R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19566R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19576R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate |
FEP |
|
Arlon 23234R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 25122R040 0.040" (1.02 mm) Silicone Rubber on Laminated Fluoropolymer Film |
Silicone Rubber |
|
Arlon 25122R060 0.060" (1.52 mm) Silicone Rubber on Laminated Fluoropolymer Film |
Silicone Rubber |
|
Arlon 25188T010 Silicone Rubber/Laminated ETFE Film |
Silicone Rubber |
|
Arlon 25188T017 Silicone Rubber/Laminated ETFE Film |
Silicone Rubber |
|
Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film |
ETFE/ECTFE |
|
Arlon 25662T010 0.010" (0.254 mm) Cured Silicone Rubber with Laminated ETFE Film Substrate |
Silicone Rubber |
|
Arlon 26122P020 0.020" Cured Silicone Rubber/Laminated PTFE Film |
PTFE |
|
Arlon 27122T125 Cured Silicone Rubber/Skive Tape Laminate |
Silicone Rubber |
|
Arlon 28540R015 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone Rubber |
|
Arlon 28561R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 28561R015M 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 28571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 28601M015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 28601W015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 28941C015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 30090R022 0.022" (0.559 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier |
Silicone Rubber |
|
Arlon 30300R062 0.062" (1.57 mm) Uncured Silicone Rubber on Kodacel Carrier |
Silicone Rubber |
|
Arlon 30400N060 0.060" (1.52 mm) Uncured Silicone Rubber |
Silicone Rubber |
|
Arlon 30400N085 0.085" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier |
Silicone Rubber |
|
Arlon 30400N125 0.125" (3.17 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier |
Silicone Rubber |
|
Arlon 30400R040 0.04" Uncured, Unsupported Silicone Rubber on Release Carrier |
Silicone Rubber |
|
Arlon 30400R060 0.06" Uncured, Unsupported Silicone Rubber on Release Carrier |
Silicone Rubber |
|
Arlon 30540R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier |
Silicone Rubber |
|
Arlon 30560R015 0.015" (0.381 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier |
Silicone Rubber |
|
Arlon 30570R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier |
Silicone Rubber |
|
Arlon 30570R015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier |
Silicone Rubber |
|
Arlon 30570R020 0.020" (0.508 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier |
Silicone Rubber |
|
Arlon 30570XA015 0.015" (0.381mm) Uncured/Unsupported Silicone Rubber on a Release Carrier |
Silicone Rubber |
|
Arlon 31570R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a HDPE Carrier |
Silicone Rubber |
|
Arlon 31570R025 0.025" (0.635 mm) Uncured Unsupported Silicone on a HDPE Carrier |
Silicone Rubber |
|
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier |
Silicone Rubber |
|
Arlon 31970XA015 Silicone Rubber Laminate |
Silicone Rubber |
|
Arlon 32090R028 Silicone Rubber Laminate |
Silicone Rubber |
|
Arlon 32140R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier |
Silicone Rubber |
|
Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier |
Silicone Rubber |
|
Arlon 32570R040 0.040" (1.02 mm) Uncured Silicone Rubber with Fiberglass Carrier |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 32580B035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier |
Silicone Rubber |
|
Arlon 32580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a PET Carrier |
Silicone Rubber |
|
Arlon 32580R020 0.020" (0.508 mm) Uncured Silicone Rubber on Polyester Film Carrier |
Silicone Rubber |
|
Arlon 32580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on PET Carrier |
Silicone Rubber |
|
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier |
Silicone Rubber |
|
Arlon 32980X040 0.040" Uncured Silicone Rubber on Polyester Film |
Silicone Rubber |
|
Arlon 32980X050 0.050" Uncured Silicone Rubber on Polyester Film |
Silicone Rubber |
|
Arlon 32980X060 0.060" Uncured Silicone Rubber on Polyester Film |
Silicone Rubber |
|
Arlon 32980XA015 0.015" Uncured Silicone Rubber on Polyester Film |
Silicone Rubber |
|
Arlon 41300R062 0.062" Uncured Silicone Rubber on Holland Cloth |
Silicone Rubber |
|
Arlon 41400R030 0.030" Uncured, Unsupported Silicone Rubber on a Release Carrier |
Silicone Rubber |
|
Arlon 41570R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier |
Silicone Rubber |
|
Arlon 41580R015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier |
Silicone Rubber |
|
Arlon 48101R008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 48106R008 0.008" (0.203 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 48366X007 0.007" (0.178 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 48571R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 48576R005 0.0055" (0.140 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 49442R0075EP 0.0075" (0.190 mm) Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 49581B010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 49581R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 49581X010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 49583R010 0.0105" (0.267 mm) Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 51073R031 0.0311" (0.79 mm) Cured Silicone Rubber with Fiberglass Substrate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 51106R015 Silicone Rubber/Fiberglass Laminate |
Silicone, Molded, Glass Fiber Filled |
|
Arlon 51106RB015D Silicone Rubber/Fiberglass Laminate |
Silicone, Molded, Glass Fiber Filled |
|