Arlon 10292R062 Cured Silicone Rubber (Unsupported) with Polyethylene Liner

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 10292R062 Cured Silicone Rubber (Unsupported) with Polyethylene Liner.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction:Material: Cured Silicone RubberLiner: PolyethyleneRecommended Cure Cycle: Product delivered curedRecommended Post Cure Cycle: Product delivered post-curedAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Liner; Arlon SQA-TMS-003
1570 microns
62.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Silicone Property; ASTM D2240
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Elongation at Break 450 %
450 %
Silicone Property; ASTM D412
Tear Strength 9.64 kN/m
55.0 pli
Silicone Property; ASTM D624
Compression Set 10 %
10 %
Silicone Property; Arlon SQA-TMS-017
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Total Product Weight (oz/yd2) 63
Arlon SQA-TMS-025